Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.0 - 95.0 µm/m-°C @Temperature >=162 °C |
7.22 - 52.8 µin/in-°F @Temperature >=324 °F |
Average value: 54.0 µm/m-°C Grade Count:1 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported .. |
|||
CTE, linear | 4.00 - 95.1 µm/m-°C | 2.22 - 52.8 µin/in-°F | Average value: 55.2 µm/m-°C Grade Count:26 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
CTE, linear | 80.0 - 95.0 µm/m-°C @Temperature 20.0 °C |
44.4 - 52.8 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
GEHR Plastics PA 6.6 Nylon 6.6, Dry Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be .. |
|||
CTE, linear | 90.0 - 95.0 µm/m-°C @Temperature 20.0 °C |
50.0 - 52.8 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-3 Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140.. |
|||
CTE, linear | 43.2 - 95.0 µm/m-°C | 24.0 - 52.8 µin/in-°F | Average value: 58.8 µm/m-°C Grade Count:4 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear | 17.0 - 95.0 µm/m-°C @Temperature 50.0 - 250 °C |
9.44 - 52.8 µin/in-°F @Temperature 122 - 482 °F |
Average value: 45.7 µm/m-°C Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |