Thermal Properties Metric English Comments
CTE, linear -2.00 - 5.00 µm/m-°C

@Temperature 55.0 - 320 °C
-1.11 - 2.78 µin/in-°F

@Temperature 131 - 608 °F
Average value: 1.79 µm/m-°C Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
CTE, linear -2.00 - 5.00 µm/m-°C

@Thickness 2.00 - 4.00 mm
-1.11 - 2.78 µin/in-°F

@Thickness 0.0787 - 0.157 in
Average value: 1.79 µm/m-°C Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
CTE, linear 1.00 - 5.00 µm/m-°C
0.556 - 2.78 µin/in-°F
(x-y)
GrafTech GRAFCELL® FFP-100 SERIES Flow Field Plate Graphite
Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid..
CTE, linear 1.00 - 5.00 µm/m-°C
0.556 - 2.78 µin/in-°F
(x-y)
GrafTech GRAFCELL® FFP-200 SERIES Flow Field Plate Graphite
Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid..
CTE, linear 1.00 - 5.00 µm/m-°C
0.556 - 2.78 µin/in-°F
(x-y)
GrafTech GRAFCELL® FFP-300 SERIES Flow Field Plate Graphite
Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid..
CTE, linear 4.00 - 5.00 µm/m-°C
2.22 - 2.78 µin/in-°F
Master Bond EP17HT-3 One component, snap-curing epoxy system
Product Description: Master Bond Polymer System EP17HT-3 is a one part epoxy that fully cures in 2-3 minutes at 250-300°F. It is capable of service up to +400°F with excellent strength retention p..
CTE, linear 4.60 - 5.00 µm/m-°C

@Temperature 20.0 - 1000 °C
2.56 - 2.78 µin/in-°F

@Temperature 68.0 - 1830 °F
Goodfellow Tungsten Carbide/Cobalt
Tungsten Carbide is a hard, brittle ceramic which, when combined with 6% to 10% Cobalt, forms a tough Cermet (Ceramic-Metal). This material was developed for use in cutting tools, having hard cerami..
CTE, linear 4.00 - 5.00 µm/m-°C

@Temperature 1000 °C
2.22 - 2.78 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CUN-50S Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 4.00 - 5.00 µm/m-°C

@Temperature 1000 °C
2.22 - 2.78 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CUN-669 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 4.00 - 5.00 µm/m-°C

@Temperature 1000 °C
2.22 - 2.78 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CUN-738 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 4.00 - 5.00 µm/m-°C

@Temperature 1000 °C
2.22 - 2.78 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CUN-804 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 4.00 - 5.00 µm/m-°C

@Temperature 1000 °C
2.22 - 2.78 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CUN-810 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 4.00 - 5.00 µm/m-°C

@Temperature 1000 °C
2.22 - 2.78 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CUN-B817 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 4.00 - 5.00 µm/m-°C

@Temperature <=1000 °C
2.22 - 2.78 µin/in-°F

@Temperature <=1830 °F
Acerde Silicon Carbide
Silicon Carbide key properties: High oxidation resistance, High hardness, Resistive to thermal stress, High thermal conductivity, Low thermal expansion, High elastic modulus, Superior chemical inert..