Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 119 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
CTE, linear | 119 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
CTE, linear | 119 µm/m-°C | 66.1 µin/in-°F | Above Tg |
Tra-Con Tra-Cast 3110 Low Density Epoxy Casting System TRA-CAST 3110 is a unicellular, low density, syntactic-foam epoxy resin casting system of medium viscosity that easily handles, mixes and cures at room temperature. Developed for industrial encapsul.. |
|||
CTE, linear | 119 µm/m-°C @Temperature 20.0 °C |
66.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-65D Polyester based. Excellent oil and chemical resistance. Applications include: Caster wheels, Seals, Gaskets, Animal tags, Hose jacketing, Ski boots, AutomotiveDat.. |