Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 °C |
5.00 µin/in-°F @Temperature 68.0 °F |
|
Potters Industries Spheriglass® 2530 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 °C |
5.00 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9294 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9300 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9338 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9348 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 30.0 - 300 °C |
5.00 µin/in-°F @Temperature 86.0 - 572 °F |
|
Novum Glass Solid Soda-lime Technical Series Glass Microspheres Solid soda-lime glass microspheres in colorless powder form. Technical Series Microspheres are solid glass microspheres that have a narrow particle size distribution. Used for chromatography, colum.. |
|||
CTE, linear | 9.00 - 12.0 µm/m-°C @Temperature -40.0 - 125 °C |
5.00 - 6.67 µin/in-°F @Temperature -40.0 - 257 °F |
IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform.. |
|||
CTE, linear | 9.00 - 30.0 µm/m-°C | 5.00 - 16.7 µin/in-°F | Average value: 14.1 µm/m-°C Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1301-8400 PPS, linear, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 30.0 - 300 °C |
5.00 µin/in-°F @Temperature 86.0 - 572 °F |
|
Mo-Sci Corporation GL-0191 Soda-Lime Glass Spheres Appearance: Solid soda-lime glass beads with light green color in powder formTypical applications of GL0191 beads include: spacer material for gauge control, coating, filler for plastic, retroreflec.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 30.0 - 300 °C |
5.00 µin/in-°F @Temperature 86.0 - 572 °F |
|
Mo-Sci Corporation GL-0262 Ni Coated Soda-Lime Glass Spheres Appearance: Solid soda-lime glass microspheres with metallic nickel coatingTypical applications of GL-0262 glass microspheres include: conductive filler for plastic, pigment, and etc.Information pro.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 30.0 - 300 °C |
5.00 µin/in-°F @Temperature 86.0 - 572 °F |
|
Mo-Sci Corporation GL-0279 Silver Coated Soda-Lime Glass Spheres Appearance: Solid soda-lime glass microspheres with metallic silver coating.Typical applications of GL0279 beads including: conductive filler for plastic, pigment, and etc.Information provided by Mo.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-0699 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1301-0825 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 100 °C |
5.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + Annealed This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + Annealed (705°C/1hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6. .. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 100 °C |
5.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 100 °C |
5.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Typical This entry has typical property data. Other database entries for TIMETAL® 6-2-4-6 have tensile and fatigue data for specific sample conditions.High-Strength, Intermediate Temperature AlloyFeatures.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 °C |
5.00 µin/in-°F @Temperature 68.0 °F |
|
Cytec Thornel® VCB-20 Carbon Cloth/Epoxy Composite Data provided by the manufacturer, Amoco Performance Products, Inc. Cured ply 0.47 mm thick, 55% fiber vol.Thornel® products were sold by Amoco and are now owned by Cytec. |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-7 Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-7B Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | y direction |
Arlon AD430 Glass, PTFE and Micro-Dispersed Ceramic High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 950 °C |
5.00 µin/in-°F @Temperature 68.0 - 1740 °F |
|
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)
(Unverified Data**) Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp.. |
|||
CTE, linear | 9.00 - 162 µm/m-°C | 5.00 - 90.0 µin/in-°F | Average value: 46.3 µm/m-°C Grade Count:23 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 1250 °C |
5.00 µin/in-°F @Temperature 68.0 - 2280 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |