Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Network Polymers NPP 908 Description: Polyester CopolymerInformation provided by Network Polymers Inc. |
|||
CTE, linear | 75.6 - 75.6 µm/m-°C @Temperature 16.0 - 16.0 °C |
42.0 - 42.0 µin/in-°F @Temperature 60.8 - 60.8 °F |
Average value: 75.6 µm/m-°C Grade Count:1 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 16.0 °C |
42.0 µin/in-°F @Temperature 60.8 °F |
R&H P-4 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast Poly 2000 (Mil-P-25690;Class 1) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast Poly 2000 (Mil-P-25690;Class 2) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast Poly 76 (Mil-P-8184) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast Poly 84 (Mil-P-8184) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast Poly 900 (DTD-5592-UK) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast Poly II (Mil-P-5425) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast SAR (Super Abrasion Resistant) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast SAR HP 1.25 (UL 752 Level 3) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast Solarcryl (0.187") Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast UF3 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast UF96 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polycast UVT (Ultra-Violet Transmitting) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R21 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R24 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R26 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R52 PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R84 Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R84/21 Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R910 PC/ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Solarex® SV Copolyester Sheet Description: Copolyester SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech SP-9070 ABS/PVC Flame Retardant Sheet Description: Flame Retardant SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 µm/m-°C @Temperature -40.0 - 37.8 °C |
42.0 µin/in-°F @Temperature -40.0 - 100 °F |
ASTM E831 |
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed.. |
|||
CTE, linear | 75.6 µm/m-°C | 42.0 µin/in-°F | |
BCC Products BC 7062-3H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R12 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 166 µm/m-°C | 42.0 - 92.2 µin/in-°F | Average value: 117 µm/m-°C Grade Count:6 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |