Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.00 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
2.22 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP545 Carbon Fiber
(discontinued **) Description: NP545 is composed of carbon fiber fabric and an epoxy resin system. It has excellent moisture resistance and physical properties. Potential uses include fixtures and gage systems, high .. |
|||
CTE, linear | 4.00 - 95.1 µm/m-°C | 2.22 - 52.8 µin/in-°F | Average value: 55.2 µm/m-°C Grade Count:26 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
CTE, linear | 4.00 - 275 µm/m-°C | 2.22 - 153 µin/in-°F | Average value: 62.6 µm/m-°C Grade Count:110 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 4.00 - 11.0 µm/m-°C | 2.22 - 6.11 µin/in-°F | |
MarkeTech Yttrium aluminum perovskite:Cerium (YAP:Ce; YAlO3) Scintillator Crystal Yttrium aluminum perovskite activated by cerium is a fast, mechanically strong and chemically resistant scintillation material. Mechanical properties enable precise machining and entrance windows ca.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature -50.0 - 50.0 °C |
2.22 µin/in-°F @Temperature -58.0 - 122 °F |
|
Mateck Fused Silica IR Grade (SiO2) Optical crystals |
|||
CTE, linear | 4.00 µm/m-°C @Temperature -50.0 - 50.0 °C |
2.22 µin/in-°F @Temperature -58.0 - 122 °F |
|
Mateck Fused Silica UV-VIS Grade (SiO2) Optical crystals |
|||
CTE, linear | 4.00 µm/m-°C @Temperature -30.0 - 70.0 °C |
2.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott G018-307 Dental Glass Remarks: Zr-containing, very low refractive indexApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided .. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature -30.0 - 70.0 °C |
2.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott GM27884 Dental Glass Remarks: Ba-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SC.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 1000 °C |
2.22 µin/in-°F @Temperature 1830 °F |
|
UBE Tyranno Grade ZMI Ceramic High Temperature Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C | 2.22 - 2.78 µin/in-°F | |
Master Bond EP17HT-3 One component, snap-curing epoxy system Product Description: Master Bond Polymer System EP17HT-3 is a one part epoxy that fully cures in 2-3 minutes at 250-300°F. It is capable of service up to +400°F with excellent strength retention p.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 20.0 - 400 °C |
2.22 µin/in-°F @Temperature 68.0 - 752 °F |
|
Zircar Refractory Composites RS-99-45 Refractory Sheet ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 20.0 - 400 °C |
2.22 µin/in-°F @Temperature 68.0 - 752 °F |
|
Zircar Refractory Composites RS-99-60 Refractory Sheet ZRCI Refractory Sheet Type RS-99-60 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 1000 °C |
2.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories BPR-DS Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 1000 °C |
2.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories BTN-2 Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 1000 °C |
2.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories COD-1 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 1000 °C |
2.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CRAG-S50 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C @Temperature 1000 °C |
2.22 - 2.78 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-50S Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C @Temperature 1000 °C |
2.22 - 2.78 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-669 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C @Temperature 1000 °C |
2.22 - 2.78 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-738 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C @Temperature 1000 °C |
2.22 - 2.78 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-804 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C @Temperature 1000 °C |
2.22 - 2.78 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-810 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 8.50 µm/m-°C @Temperature 1000 °C |
2.22 - 4.72 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-846 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C @Temperature 1000 °C |
2.22 - 2.78 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-B817 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 1000 °C |
2.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories ZR-C Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C @Temperature <=1000 °C |
2.22 - 2.78 µin/in-°F @Temperature <=1830 °F |
|
Acerde Silicon Carbide Silicon Carbide key properties: High oxidation resistance, High hardness, Resistive to thermal stress, High thermal conductivity, Low thermal expansion, High elastic modulus, Superior chemical inert.. |
|||
CTE, linear | 4.00 µm/m-°C | 2.22 µin/in-°F | In Plane; ASTM E289-95 |
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl.. |
|||
CTE, linear | 4.00 - 55.8 µm/m-°C | 2.22 - 31.0 µin/in-°F | Average value: 26.3 µm/m-°C Grade Count:21 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
CTE, linear | 4.00 - 500 µm/m-°C @Temperature 55.0 - 160 °C |
2.22 - 278 µin/in-°F @Temperature 131 - 320 °F |
Average value: 376 µm/m-°C Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |