Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
|
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-40-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-40-30 Cellular Urethane Foam Information on this material is preliminary.Standard color is black (04); others are available. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F).General Poron® information: Poron® fo.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-41-15 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-41-20 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-41-30 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-50 Thin as Cast Urethane Foam, Firm, Thin as Cast Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-60-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-60-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-60-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4790-92-20 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
CTE, linear | 230 µm/m-°C @Temperature 20.0 °C |
128 µin/in-°F @Temperature 68.0 °F |
dilatation; ASTM D696 |
Petroquimica Triunfo Trithene® JX 7065 LDPE - Injection Molding and Master Batch The Trithene® JX 7065 resin is a low-density polyethylene with a wide molecular weight distribution, developed to offer good impact resistance, excellent flexibility, and high resistance to stress .. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
CTE, linear | 230 µm/m-°C @Temperature 20.0 °C |
128 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials TSE3033 Clear General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
CTE, linear | 230 µm/m-°C | 128 µin/in-°F | Above Tg |
Tra-Con Tra-Duct 916H03 Room Temperature Cure High Conductivity Silver Epoxy Adhesive TRA-DUCT 916H03 is recommended for electronic bonding and sealing applications that require the combination of high conductivity coupled with good mechanical properties. This two part smooth paste s.. |
|||
CTE, linear | 231 µm/m-°C | 128 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 353ND-T Black High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T Black is a two component, high temperature, thixotropic epoxy for fiber optic, PCB and various medical applications. Advantages & Application Notes: This produ.. |
|||
CTE, linear | 231 µm/m-°C | 128 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 353ND-T High Temperature Thixotropic Epoxy Product Description: EPO TEK® 353ND-T is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. Advantages & Application Notes: Suitable for fiber op.. |
|||
CTE, linear | 231 µm/m-°C | 128 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 353ND-T1 High Temperature Thixotropic Epoxy Material Description: A two component, thixotropic and high temperature epoxy designed for fiber optic, electronics and medical applications. It is a more viscous alternative to EPO-TEK® 353ND-T.I.. |
|||
CTE, linear | 231 µm/m-°C | 128 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 353ND-T5 High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T5 is an intermediate viscosity version of EPO-TEK® 353ND and EPO-TEK® 353ND-T. It was designed for high temperature applications in fiber optics, electronics .. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-40-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-50-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |