Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 220 µm/m-°C @Thickness 2.00 mm, Temperature -125 - 20.0 °C |
122 µin/in-°F @Thickness 0.0787 in, Temperature -193 - 68.0 °F |
ASTM E831-06 |
NeXolve Essar™ Stretch 255 Polyimide High temperature colorless elastic polyimide. NeXolve Essar™ Stretch 255 combines polyimide high temperature survivability and stability with elastomer elasticity and optical clarity into a single .. |
|||
CTE, linear | 220 µm/m-°C @Temperature 20.0 °C |
122 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV511 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DEBT (deputy tin deflagrate) as the stan.. |
|||
CTE, linear | 220 µm/m-°C @Temperature 20.0 °C |
122 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV511 White Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
CTE, linear | 220 - 240 µm/m-°C | 122 - 133 µin/in-°F | |
Master Bond MasterSil 151Med Medical Grade Silicone Potting Compound Description: Master Bond MasterSil 151Med is a two component, low viscosity silicone compound for high performance potting and encapsulation. MasterSil 151Med is an addition cured system and does no.. |
|||
CTE, linear | 219 µm/m-°C | 122 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy Material Description: Silver-filled, electrically conductive, flexible epoxyInformation Provided by Epoxy Technology |
|||
CTE, linear | 220 µm/m-°C @Temperature 30.0 - 150 °C |
122 µin/in-°F @Temperature 86.0 - 302 °F |
Silicone Property; ASTM E 831 |
Arlon CP-RC-3916 Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
CTE, linear | 219 µm/m-°C | 122 µin/in-°F | above Tg |
3M Scotch-Weld™ DP605NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properl.. |