Polymer Property : CTE, linear = 99.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 99.0 - 99.0 µm/m-°C

@Temperature 22.8 - 55.0 °C
55.0 - 55.0 µin/in-°F

@Temperature 73.0 - 131 °F
Average value: 99.0 µm/m-°C Grade Count:1
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
CTE, linear 63.1 - 99.0 µm/m-°C
35.1 - 55.0 µin/in-°F
Average value: 74.4 µm/m-°C Grade Count:9
Overview of materials for PVC, Sheet Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M..
CTE, linear 36.0 - 99.0 µm/m-°C
20.0 - 55.0 µin/in-°F
Average value: 64.3 µm/m-°C Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Wood Filled". Each property range of values reported is minimum and ma..
CTE, linear 43.0 - 99.0 µm/m-°C

@Temperature 40.0 - 130 °C
23.9 - 55.0 µin/in-°F

@Temperature 104 - 266 °F
Average value: 62.3 µm/m-°C Grade Count:22
Overview of materials for Phenolic, Novolac, Woodflour Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum valu..
CTE, linear 82.8 - 99.0 µm/m-°C

@Temperature 20.0 °C
46.0 - 55.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Royalite DKE 400 PVC/Acrylic Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
CTE, linear 82.8 - 99.0 µm/m-°C

@Temperature 20.0 °C
46.0 - 55.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Royalite R47 PVC Alloy Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
CTE, linear 82.8 - 99.0 µm/m-°C

@Temperature 20.0 °C
46.0 - 55.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Royalite R57 FR/ABS Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
CTE, linear 82.8 - 99.0 µm/m-°C

@Temperature 20.0 °C
46.0 - 55.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Royalite R570 FR-ABS Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
CTE, linear 82.8 - 99.0 µm/m-°C

@Temperature 20.0 °C
46.0 - 55.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Royalite R59 ABS/PVC Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
CTE, linear 82.8 - 99.0 µm/m-°C

@Temperature 20.0 °C
46.0 - 55.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Royalite R66 PVC/Acrylic Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
CTE, linear 82.8 - 99.0 µm/m-°C

@Temperature 20.0 °C
46.0 - 55.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Royalite R71/920 PC/ABS Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
CTE, linear 82.8 - 99.0 µm/m-°C

@Temperature 20.0 °C
46.0 - 55.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Royalite R87/59 ABS/PVC Weather Resistant Sheet
Description: Weather Resistant SheetInformation provided by Spartech.
CTE, linear 40.0 - 99.0 µm/m-°C
22.2 - 55.0 µin/in-°F
Average value: 57.4 µm/m-°C Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
CTE, linear 82.8 - 99.0 µm/m-°C

@Temperature 20.0 °C
46.0 - 55.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Royalite R60-LS (R61) PVC/Acrylic Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.