Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 55.0 - 162 µm/m-°C | 30.6 - 90.0 µin/in-°F | Average value: 87.4 µm/m-°C Grade Count:106 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
CTE, linear | 72.0 - 162 µm/m-°C @Temperature 25.6 - 204 °C |
40.0 - 90.0 µin/in-°F @Temperature 78.0 - 400 °F |
ASTM D696 |
Technetics Group Texolon™ 7865 PTFE
(Unverified Data**) Virgin PTFE for those applications not requiring the premium qualities of 8764 sheet.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surfac.. |
|||
CTE, linear | 72.0 - 162 µm/m-°C @Temperature 25.6 - 204 °C |
40.0 - 90.0 µin/in-°F @Temperature 78.0 - 400 °F |
ASTM D696 |
Garlock 8764 PTFE Rubber Sheet Premium Grade Skived PTFE SheetInformation provided by Garlock Rubber Technologies |
|||
CTE, linear | 72.0 - 162 µm/m-°C @Temperature 25.6 - 204 °C |
40.0 - 90.0 µin/in-°F @Temperature 78.0 - 400 °F |
ASTM D696 |
Technetics Group Texolon™ 8764 PTFE
(Unverified Data**) A premium PTFE sheet manufactured from the highest quality PTFE.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectri.. |
|||
CTE, linear | 9.00 - 162 µm/m-°C | 5.00 - 90.0 µin/in-°F | Average value: 46.3 µm/m-°C Grade Count:23 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |