Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 96.0 µm/m-°C @Temperature -30.0 - 100 °C |
53.3 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
LyondellBasell Hifaxâ„¢ ETA-3104HF Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus thermoplastic elastomeric olefin resin, good impact and stiffness balance, good dimensional stability, good processabilityApplications: molded-in color.. |
|||
CTE, linear | 96.0 µm/m-°C | 53.3 µin/in-°F | ISO 11359-2 |
Unitika A1030BRL PA6, Conditioned Information provided by Unitika Ltd. |
|||
CTE, linear | 96.0 µm/m-°C | 53.3 µin/in-°F | ISO 11359-2 |
Unitika A1030BRL PA6, Dry Information provided by Unitika Ltd. |
|||
CTE, linear | 96.0 µm/m-°C | 53.3 µin/in-°F | ISO 11359-2 |
Unitika A1030FR PA6, Conditioned Information provided by Unitika Ltd. |
|||
CTE, linear | 96.0 µm/m-°C | 53.3 µin/in-°F | ISO 11359-2 |
Unitika A1030FR PA6, Dry Information provided by Unitika Ltd. |
|||
CTE, linear | 96.0 µm/m-°C | 53.3 µin/in-°F | ISO 11359-2 |
Unitika A1030JR PA6, Conditioned Information provided by Unitika Ltd. |
|||
CTE, linear | 96.0 µm/m-°C | 53.3 µin/in-°F | ISO 11359-2 |
Unitika A1030SR PA6, Dry Information provided by Unitika Ltd. |
|||
CTE, linear | 96.0 µm/m-°C | 53.3 µin/in-°F | ISO 11359-2 |
Unitika A1030JR PA6, Dry Information provided by Unitika Ltd. |
|||
CTE, linear | 96.0 µm/m-°C | 53.3 µin/in-°F | ISO 11359-2 |
Unitika A1030SR PA6, Conditioned Information provided by Unitika Ltd. |
|||
CTE, linear | 96.0 µm/m-°C | 53.3 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy Product Description: EPO-TEK® 354 is a two component, high Tg epoxy designed for semiconductor packaging in medical, fiber optic and optoelectronic assemblies. It is an electrically and thermally i.. |