Polymer Property : CTE, linear = 61.2 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 61.2 µm/m-°C

@Temperature 20.0 °C
34.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Lubri-Tech™ PF-000/15T Polysulfone, PTFE Lubricated  (discontinued **)
Description/Features:PTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
CTE, linear 61.2 µm/m-°C

@Temperature 20.0 °C
34.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
ITW Devcon Metal Repair Stainless Steel Putty (ST), Grey
Information provided by ITW Devcon
CTE, linear 61.2 µm/m-°C

@Temperature 20.0 °C
34.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
ITW Devcon Plastic Steel® Metal Repair 5 Minute® Putty (SF), Dark Grey
Information provided by ITW Devcon
CTE, linear 61.2 µm/m-°C
34.0 µin/in-°F
ASTM D696
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced
Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex
CTE, linear 61.2 µm/m-°C
34.0 µin/in-°F
ASTM D696
Teknor Apex Chemlon® 212 Nylon 6, Unreinforced
Features: Lubricated, General Purpose; General purpose nylon 6; Slightly tougher and more ductile than nylon 66 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex..
CTE, linear 61.2 µm/m-°C

@Temperature 20.0 °C
34.0 µin/in-°F

@Temperature 68.0 °F
ASTM D1525
PlastxWorld CEVIAN® S1210 PC/ABS alloy
Glass fiber reinforced PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
CTE, linear 61.2 µm/m-°C
34.0 µin/in-°F
ASTM D696
Ensinger Hydex™ 301 Rigid Polyurethane (PU)
Hydex™ 301 is clear totally rigid polyurethane. It combines excellent clarity when polished with a broad range of chemical resistance and outstanding practical toughness.
CTE, linear 61.2 - 108 µm/m-°C
34.0 - 60.0 µin/in-°F
Average value: 84.7 µm/m-°C Grade Count:13
Overview of materials for Nylon 6, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate..