Polymer Property : CTE, linear = 6.70 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.70 µm/m-°C

@Temperature 20.0 °C
3.72 µin/in-°F

@Temperature 68.0 °F
GBC Grade 85 Alumina
Data provided by the manufacturer, GBC Materials Corporation.
CTE, linear 6.70 µm/m-°C

@Temperature 20.0 °C
3.72 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials Zirconium Carbide (ZrC) Coating
High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i..
CTE, linear 6.70 µm/m-°C

@Temperature 1000 °C
3.72 µin/in-°F

@Temperature 1830 °F
Chosun Refractories AC-2 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 6.70 µm/m-°C
3.72 µin/in-°F
Esstech V-116-1130 Barium Silicate Glass
Barium Silicate glass is an inorganic filler with a high refractive index of 1.580. It also has a high coefficient of thermal expansion and a high barium content, which increases its x-ray opacity. ..
CTE, linear 6.70 µm/m-°C

@Temperature 1000 °C
3.72 µin/in-°F

@Temperature 1830 °F
COI Ceramics Friable Graded Insulation
Description: An example of a bonded product comprised of oxide spheres is Friable Graded Insulation or FGI. FGI can be bonded to an oxide ceramic matrix composite such as A/N720 to produce a CMC/FGI..
CTE, linear 6.70 µm/m-°C

@Temperature 27.0 - 175 °C
3.72 µin/in-°F

@Temperature 80.6 - 347 °F
ASTM D696
3M 7953MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
CTE, linear 6.70 µm/m-°C
3.72 µin/in-°F
Plansee MoCu15 Molybdenum-Copper
Characteristics:High thermal conductivityLow thermal expansionLow densityApplications:Electronic components - passive cooling elementsAutomotive industry - carrier plates for IGBT modules in electri..
CTE, linear 6.70 µm/m-°C

@Temperature 20.0 - 200 °C
3.72 µin/in-°F

@Temperature 68.0 - 392 °F
CeramTec 433 Alumina, 99.9%
433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A ..
CTE, linear 6.70 µm/m-°C
3.72 µin/in-°F
parallel C-axis
Mateck Sapphire Aluminium oxide Substrate, Al2O3
Substrate single crystals for superconductivity.
Copyright © lookpolymers.com All Rights Reserved