Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 3.60 µm/m-°C @Temperature 20.0 °C |
2.00 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Owens Corning Glass Fiber Reinforced Epoxy (Filament Wound), 80 wt.% glass Epoxies are highly resistant to water, alkalis and organic solvents. Although standard epoxies have only a fair resistance to acids and oxidizing agents, they can be formulated for better resistance.. |
|||
CTE, linear | 3.60 µm/m-°C @Temperature 20.0 °C |
2.00 µin/in-°F @Temperature 68.0 °F |
TMA |
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC Lytex 4149 is a high-performance, 3K tow carbon fiber (PAN) reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical propert.. |
|||
CTE, linear | 3.60 - 72.0 µm/m-°C | 2.00 - 40.0 µin/in-°F | Average value: 25.9 µm/m-°C Grade Count:38 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
CTE, linear | 3.60 µm/m-°C | 2.00 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h.. |
|||
CTE, linear | 3.60 µm/m-°C @Temperature 23.0 - 85.0 °C |
2.00 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® 2412GHF8 PA66, 40% glass fiber, DRY Description: Polyamid 66, reinforced with 40% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF8 is used in all sectors of indu.. |
|||
CTE, linear | 3.60 µm/m-°C @Temperature 20.0 - 100 °C |
2.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
UCAR Carbon UCAR® PGW Pressure Molded Graphite An economical low ash material with excellent thermal shock resistance, Grade PGW is well suited for the fine machining detail required in molds for casting metal shapes. Grade PGW is a molded versi.. |
|||
CTE, linear | 3.60 - 47.0 µm/m-°C | 2.00 - 26.1 µin/in-°F | Average value: 24.7 µm/m-°C Grade Count:19 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
CTE, linear | 3.60 µm/m-°C @Temperature 20.0 - 1000 °C |
2.00 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Ceradyne Ekatherm EKasin® S Gas Pressure Sintered Silicon Nitride (Si3N4) EKatherm® Silicon Nitride is the state-of-the-art material for a wide variety of components used in Aluminum Alloy casting processes.Features: High Temperature Resistance High Thermal Shock Resist.. |
|||
CTE, linear | 3.60 µm/m-°C | 2.00 µin/in-°F | |
Aremco Ceramacast™ 905 Silicon-Ceramic Potting Compound Ceramacast™ 905 is a silicone-bonded, ceramic filled high temperature adhesive and potting compound. |