Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 3.00 - 110 µm/m-°C | 1.67 - 61.1 µin/in-°F | Average value: 23.2 µm/m-°C Grade Count:47 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 20.0 - 1000 °C |
1.67 µin/in-°F @Temperature 68.0 - 1830 °F |
|
McDanel Advanced Ceramics SiAlON Information provided by McDanel Advanced Ceramic Technologies. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 20.0 - 750 °C |
1.67 µin/in-°F @Temperature 68.0 - 1380 °F |
BSÂ 1902: section 5.3: 1990 |
Skamol Group Moler HIPOROS Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 20.0 - 750 °C |
1.67 µin/in-°F @Temperature 68.0 - 1380 °F |
BSÂ 1902: section 5.3: 1990 |
Skamol Group Moler LR-1750 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 20.0 - 750 °C |
1.67 µin/in-°F @Temperature 68.0 - 1380 °F |
BSÂ 1902: section 5.3: 1990 |
Skamol Group Moler M-EXTRA 'E' Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 20.0 - 750 °C |
1.67 µin/in-°F @Temperature 68.0 - 1380 °F |
BSÂ 1902: section 5.3: 1990 |
Skamol Group Moler ROTOL Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 20.0 °C |
1.67 µin/in-°F @Temperature 68.0 °F |
|
Sapco C 410 Steatite Information provided by Sapco. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature -30.0 - 70.0 °C |
1.67 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott G018-163 Dental Glass Remarks: Sr- and F-containing, very low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Pr.. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 20.0 - 750 °C |
1.67 µin/in-°F @Temperature 68.0 - 1380 °F |
BSÂ 1902: section 5.3: 1990 |
Skamol Group Moler SM-65 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 100 °C |
1.67 µin/in-°F @Temperature 77.0 - 212 °F |
ASTM E831 |
M Cubed Technologies SSC-FG Reaction-Bonded Silicon Carbide, Fine-Grained Fine-grained reaction-bonded SiC. Used for mechanical seals and other SiC applications that require a high surface finish/tight tolerances. Si content can be tailored for the application.Informati.. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 100 °C |
1.67 µin/in-°F @Temperature 77.0 - 212 °F |
ASTM E831 |
M Cubed Technologies TSC-15 Titanium-alloyed Reaction Bonded Silicon Carbide Specialty reaction-bonded SiC for applications requiring high stiffness, high toughness, and also high thermal conductivity--mechanical seals, for example Flow-through complex channels can be forme.. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 1000 °C |
1.67 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories COD-2 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 3.00 - 4.00 µm/m-°C @Temperature 1000 °C |
1.67 - 2.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-718 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
3M Nextel™ AF-10 Aerospace Woven Fabric 312 Information provided by 3M |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
3M Nextel™ AF-10 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
3M Nextel™ AF-12 Aerospace Woven Fabric 312 Information provided by 3M |
|||
CTE, linear | 3.00 µm/m-°C | 1.67 µin/in-°F | |
Atom Adhesives AA-DUCT 905 Epoxy Adhesive AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive.. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
3M Nextel™ AF-11 Industrial Woven Fabric 312 Information provided by 3M |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
3M Nextel™ AF-12 Industrial Woven Fabric 312 Information provided by 3M |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
3M Nextel™ AF-12 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
3M Nextel™ AF-20 Industrial Woven Fabric 312 Information provided by 3M |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
3M Nextel™ AF-30 Industrial Woven Fabric 312 Information provided by 3M |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
3M Nextel™ AF-40 Industrial Woven Fabric 312 Information provided by 3M |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
3M Nextel™ AF-62 Industrial Woven Fabric 312 Information provided by 3M |
|||
CTE, linear | 3.00 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
1.67 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
3M Nextel™ 312 Industrial Ceramic Fiber Chemical composition above is wt%. Crystal phase is mullite + amorphous (or 100% amorphous). Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural appli.. |
|||
CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
3M Nextel™ AF-14 Industrial Woven Fabric 312 Information provided by 3M |