Material Notes:
Information provided by McDanel Advanced Ceramic Technologies.
Physical Properties Metric English Comments
Bulk Density 3.24 g/cc
0.117 lb/in³
Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Flexural Strength 760 MPa
110000 psi
560 MPa

@Temperature 538 °C
81200 psi

@Temperature 1000 °F
Compressive Strength 3500 MPa
508000 psi
Thermal Properties Metric English Comments
CTE, linear 3.00 µm/m-°C

@Temperature 20.0 - 1000 °C
1.67 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1200 °C
2190 °F
no load