Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 230 - 310 µm/m-°C

@Temperature 20.0 °C
128 - 172 µin/in-°F

@Temperature 68.0 °F
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
CTE, linear 230 - 310 µm/m-°C

@Temperature 20.0 °C
128 - 172 µin/in-°F

@Temperature 68.0 °F
ASTM C518
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4701-30-20064 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Contains PET film reinforcement. Standard available  thickness 0.064"Features and Benefits of PORON Products: Excelle..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
CTE, linear 230 - 310 µm/m-°C

@Temperature 20.0 °C
128 - 172 µin/in-°F

@Temperature 68.0 °F
ASTM C518
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4..
CTE, linear 230 - 310 µm/m-°C

@Temperature 20.0 °C
128 - 172 µin/in-°F

@Temperature 68.0 °F
ASTM C518
Rogers Corporation Poron® 4701-40-15 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
CTE, linear 230 - 310 µm/m-°C

@Temperature 20.0 °C
128 - 172 µin/in-°F

@Temperature 68.0 °F
ASTM C518
Rogers Corporation Poron® 4701-40-30 Cellular Urethane Foam
Information on this material is preliminary.Standard color is black (04); others are available. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F).General Poron® information: Poron® fo..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4701-41-20 Urethane Foam, Soft, Enhanced Sealability
Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements.  Standard available thickness range from 0.031"..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4701-41-30 Urethane Foam, Soft, Enhanced Sealability
Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements.  Standard available thickness range from 0.031"..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported
Firm material used for managing high energy impact with gasketing needs.  Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4701-50 Thin as Cast Urethane Foam, Firm, Thin as Cast
Firm material used for managing high energy impact with gasketing needs.  Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce..
CTE, linear 230 - 310 µm/m-°C

@Temperature 20.0 °C
128 - 172 µin/in-°F

@Temperature 68.0 °F
ASTM C518
Rogers Corporation Poron® 4701-50-15 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
CTE, linear 230 - 310 µm/m-°C

@Temperature 20.0 °C
128 - 172 µin/in-°F

@Temperature 68.0 °F
ASTM C518
Rogers Corporation Poron® 4701-50-30 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4..
CTE, linear 230 - 310 µm/m-°C

@Temperature 20.0 °C
128 - 172 µin/in-°F

@Temperature 68.0 °F
ASTM C518
Rogers Corporation Poron® 4701-60-15 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
CTE, linear 230 - 310 µm/m-°C

@Temperature 20.0 °C
128 - 172 µin/in-°F

@Temperature 68.0 °F
ASTM C518
Rogers Corporation Poron® 4701-60-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
CTE, linear 230 - 310 µm/m-°C

@Temperature 20.0 °C
128 - 172 µin/in-°F

@Temperature 68.0 °F
ASTM C518
Rogers Corporation Poron® 4701-60-30 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4790-92-12 Urethane Foam, Extra Soft, Slow Rebound
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4790-92-20 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
CTE, linear 230 µm/m-°C

@Temperature 20.0 °C
128 µin/in-°F

@Temperature 68.0 °F
dilatation; ASTM D696
Petroquimica Triunfo Trithene® JX 7065 LDPE - Injection Molding and Master Batch
The Trithene® JX 7065 resin is a low-density polyethylene with a wide molecular weight distribution, developed to offer good impact resistance, excellent flexibility, and high resistance to stress ..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab..
CTE, linear 230 - 310 µm/m-°C
128 - 172 µin/in-°F
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
CTE, linear 230 µm/m-°C

@Temperature 20.0 °C
128 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials TSE3033 Clear General Purpose Potting/Encapsulating Compound
Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth..
CTE, linear 230 µm/m-°C
128 µin/in-°F
Above Tg
Tra-Con Tra-Duct 916H03 Room Temperature Cure High Conductivity Silver Epoxy Adhesive
TRA-DUCT 916H03 is recommended for electronic bonding and sealing applications that require the combination of high conductivity coupled with good mechanical properties. This two part smooth paste s..
CTE, linear 230 - 310 µm/m-°C

@Temperature 20.0 °C
128 - 172 µin/in-°F

@Temperature 68.0 °F
ASTM C518
Rogers Corporation Poron® 4701-40-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
CTE, linear 230 - 310 µm/m-°C

@Temperature 20.0 °C
128 - 172 µin/in-°F

@Temperature 68.0 °F
ASTM C518
Rogers Corporation Poron® 4701-50-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..