Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 2.80 - 70.0 µm/m-°C | 1.56 - 38.9 µin/in-°F | Average value: 49.4 µm/m-°C Grade Count:7 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
CTE, linear | 2.80 µm/m-°C @Temperature 260 °C |
1.56 µin/in-°F @Temperature 500 °F |
|
Ferro EG 1001 Metal Sealing Glass Type: Si-B Typical Powder Form: VSD Typical Application: Gun Mount Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals for.. |
|||
CTE, linear | 2.80 µm/m-°C @Temperature 20.0 - 100 °C |
1.56 µin/in-°F @Temperature 68.0 - 212 °F |
|
UCAR Carbon UCAR® ATA Isostatic Molded Graphite Economical grade ATA is the lowest density version of isostatically molded, fine grain grade ATJ family of graphite materials.Typical Applications: ATA is used in general purpose applications where .. |
|||
CTE, linear | 2.80 µm/m-°C @Temperature 20.0 - 100 °C |
1.56 µin/in-°F @Temperature 68.0 - 212 °F |
|
UCAR Carbon UCAR® ATJ Isostatic Molded Graphite Isostatically molded ATJ has been an industry standard for many years. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish. Grade ATJ has.. |
|||
CTE, linear | 2.80 µm/m-°C @Temperature 20.0 - 100 °C |
1.56 µin/in-°F @Temperature 68.0 - 212 °F |
|
UCAR Carbon UCAR® ATR Isostatic Molded Graphite Isostatically molded ATR is a lower density version of grade ATJ. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish.Typical Application.. |
|||
CTE, linear | 2.80 µm/m-°C @Temperature 0.000 - 300 °C |
1.56 µin/in-°F @Temperature 32.0 - 572 °F |
|
Corning 7761 Potash Borosilicate Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated. |
|||
CTE, linear | 2.80 µm/m-°C | 1.56 µin/in-°F | Volumetric thermal expansion |
China-Yixing Longly Refractories Seggar SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |
|||
CTE, linear | 2.80 µm/m-°C @Temperature 27.0 - 175 °C |
1.56 µin/in-°F @Temperature 80.6 - 347 °F |
ASTM D696 |
3M 7997MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
CTE, linear | 2.80 µm/m-°C @Temperature 20.0 °C |
1.56 µin/in-°F @Temperature 68.0 °F |
|
Potters Industries Spheriglass® 3000E Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |