Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 °C |
9.50 µin/in-°F @Temperature 68.0 °F |
|
Performance Alloys MoldStar® 90 Copper Mold Alloy Description: MoldStar® 90 is a beryllium-free copper alloy for the blow molding and injection molding industries as well as other industrial applications. MoldStar® 90 provides a good balance of t.. |
|||
CTE, linear | 17.1 - 90.0 µm/m-°C | 9.50 - 50.0 µin/in-°F | Average value: 48.4 µm/m-°C Grade Count:38 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
CTE, linear | 17.1 µm/m-°C | 9.50 µin/in-°F | |
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper C18150 Chrome Copper Zirconium is recommended for spot and seam welding cold and hot-rolled steel, stainless steel and low conductivity brass and bronze. C18150 Chrome Copper Zirconium Alloy is typi.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 200 °C |
9.50 µin/in-°F @Temperature 68.0 - 392 °F |
|
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 300 °C |
9.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 64725 MAX251C, 1/2 Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 300 °C |
9.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 64725 MAX251C, Extra Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 300 °C |
9.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 64725 MAX251C, Extra Spring Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 300 °C |
9.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 64725 MAX251C, Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 300 °C |
9.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 64725 MAX251C, Spring Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 300 °C |
9.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 706 Copper Nickel 10%, 1/2 Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 300 °C |
9.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 706 Copper Nickel 10%, 1/4 Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 300 °C |
9.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 706 Copper Nickel 10%, Annealed 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 300 °C |
9.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 706 Copper Nickel 10%, Extra Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 300 °C |
9.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 706 Copper Nickel 10%, Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 300 °C |
9.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 706 Copper Nickel 10%, Spring 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 20.0 - 300 °C |
9.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Carlson 90 10 Cu Ni Copper-Nickel Alloy General DescriptionCarlson Alloy 90 10 Cu Ni is a copper-based alloy developed as a cost-effective substitute for 70 30 Cu Ni. An addition of approximately 1.4% iron was made to increase its resist.. |
|||
CTE, linear | 17.1 µm/m-°C @Temperature 21.1 - 871 °C |
9.50 µin/in-°F @Temperature 70.0 - 1600 °F |
|
Carlson C 601 Nickel-Chromium-Iron Alloy General DescriptionCarlson Alloy C 6021 is a nickel-chromium alloy, developed specifically for high –temperature service. This alloy exhibits outstanding resistance to both cyclic and static oxida.. |