Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.7 µm/m-°C @Temperature 20.0 - 100 °C |
7.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals MONEL® Alloy 401 A copper-nickel alloy designed for specialized electrical and electronic applications. It has a very low temperature coefficient of resistance and medium-range electrical resistivity. Used for wir.. |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 20.0 - 100 °C |
7.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals MONEL® Alloy K-500 A precipitation-hardenable nickel-copper alloy that combines the corrosion resistance of MONEL alloy 400 with greater strength and hardness. It also has low permeability and is nonmagnetic to under.. |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 20.0 - 100 °C |
7.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals MONEL® Alloy R-405 The free-machining version of MONEL alloy 400. A controlled amount of sulfur is added to the alloy to provide sulfide inclusions that act as chip breakers during machining. Other characteristics a.. |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 93.0 °C |
7.61 µin/in-°F @Temperature 199 °F |
|
Special Metals UDIMET® alloy D-979 Fe-Ni Alloy UDIMET® alloy D-979 (UNS N09979) is an iron-nickel alloy designed for turbine disc applications at temperatures up to 1200-1400°F (649-760°C). Hardened by a complex precipitation of interm.. |
|||
CTE, linear | 13.7 µm/m-°C | 7.60 µin/in-°F | |
Weartech International WT-694 Cobalt Hardfacing & Wear Resistant Alloy Information provided by Weartech International |
|||
CTE, linear | 13.7 µm/m-°C | 7.60 µin/in-°F | |
Weartech International WT-21 Cobalt Hardfacing & Wear Resistant Alloy Applications: hot trimming & forging dies, high pressure high temperature valves, hot shears, valve seats, pump impellers, ringsInformation provided by Weartech International |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 20.0 - 100 °C |
7.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum AL 2205™ Duplex Stainless Steel, Plate > 0.1875" Duplex Stainless Steel, UNS S31803 Ferromagnetic. The AL 2205 alloy is a nitrogen-enhanced duplex stainless steel alloy. The nitrogen serves to significantly improved the corrosion resistance of the alloy; especially in the welded c.. |
|||
CTE, linear | 13.7 µm/m-°C @Temperature 20.0 - 100 °C |
7.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum AL 2205™ Duplex Stainless Steel, Sheet and Strip < 0.1875", UNS S31803 Ferromagnetic. The AL 2205 alloy is a nitrogen-enhanced duplex stainless steel alloy. The nitrogen serves to significantly improved the corrosion resistance of the alloy; especially in the welded c.. |
|||
CTE, linear | 13.7 µm/m-°C | 7.60 µin/in-°F | |
Weartech International WT-1 Cobalt Hardfacing & Wear Resistant Alloy Applications: seaming rolls, valve seats, wear pads, pump sleeves, seals, bearings, bushings, saw blades, cuttersInformation provided by Weartech International |
|||
CTE, linear | 13.7 µm/m-°C | 7.60 µin/in-°F | |
Weartech International WT-190 Cobalt Hardfacing & Wear Resistant Alloy Applications: tri-cone rock bits for oil drillingInformation provided by Weartech International |
|||
CTE, linear | 13.7 µm/m-°C | 7.60 µin/in-°F | |
Weartech International WT-20 Cobalt Hardfacing & Wear Resistant Alloy Applications: marine engine valves, control valves for petrochemicals, steel mill rolls, homogenizer valve componentsInformation provided by Weartech International |