CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals BRIGHTRAY® Alloy 35 Electrical Resistance Alloy
A nickel-iron-chromium electrical-resistance alloy for use at operating temperatures up to 1920°F (1050°C). It is similar to BRIGHTRAY alloy F but with rare-earth additions for greater resist..
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals Nickel 212
Wrought nickel strengthened with an added manganese. Used for electrical and electronic applications such as lead wires, supporting components in lamps and cathode-ray tubes, and electrodes in glow..
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
AK Steel ASTM A 1011, Class 2 Formable, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F)
Not listed in the ASTM.Information provided by AK Steel
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
AK Steel ASTM A 424 Type III, I-F Enamel Enameling Carbon Steel
I-F Enameling Steel is a vacuum degassed, titanium stabilized steel. I-F Enameling Steel can be used for ground coat and two coat-one fire porcelain enameling systems. It is not recommended for us..
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade
Interstitial Free (I-F) steels are made by adding titanium and/or niobium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade
Interstitial Free (I-F) steels are made by adding titanium and/or niobium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade
Interstitial Free (I-F) steels are made by adding titanium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Extra Deep Drawing Steel (EDDS), Standard Grade
Interstitial Free (I-F) steels are made by adding titanium and/or columbium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade
Interstitial Free (I-F®) steels are made by adding titanium and/or columbium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade
Interstitial Free (I-F®) steels are made by adding titanium and/or columbium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
AK Steel ASTM A 1011, Class 2 Formable, Grade 50F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F)
Information provided by AK Steel
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
AK Steel ASTM A 1011, Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F)
Information provided by AK Steel
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade
Interstitial Free (I-F) steels are made by adding titanium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Extra Deep Drawing Steel Plus (EDDS+), Standard Grade
Interstitial Free (I-F) steels are made by adding titanium and/or columbium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel
Copyright © lookpolymers.com All Rights Reserved