AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel
Manufacturer AK Steel
Trade Name ZINCGRIP®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Interstitial Free (I-F®) steels are made by adding titanium and/or columbium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 310 MPa
45000 psi
.0275 - .035 inches sheet thickness; ASTM A 370
Tensile Strength, Yield 165 MPa
23900 psi
.0275 - .035 inches sheet thickness; ASTM A 370
Elongation at Break 44 %
44 %
.0275 - .035 inches sheet thickness; ASTM A 370
Modulus of Elasticity 200 GPa
29000 ksi
Thermal Properties Metric English Comments
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.481 J/g-°C

@Temperature 50.0 - 100 °C
0.115 BTU/lb-°F

@Temperature 122 - 212 °F
Thermal Conductivity 93.0 W/m-K
645 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000142 ohm-cm
0.0000142 ohm-cm
Descriptive Properties Value Comments
Deep-Drawing Capability rm 1.6
.0275 - .035 inches sheet thickness
Strain Hardening Exponent n 0.23
.0275 - .035 inches sheet thickness