Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 119 µm/m-°C @Temperature -40.0 - 149 °C |
66.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Symalit® ECTFE Ethylene-Chlorotrifluoroethylene (ASTM Product Data Sheet) |
|||
CTE, linear | 119 µm/m-°C @Temperature -40.0 - 149 °C |
66.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Symalit® PVDF (ASTM Product Data Sheet) |
|||
CTE, linear | 119 µm/m-°C | 66.0 µin/in-°F | ASTM D696 |
Quantum PVDF Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 119 - 139 µm/m-°C @Temperature 20.0 °C |
66.0 - 77.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Saint-Gobain Norton® PVDF Fluoropolymer Film Features/Benefits:Excellent weatherabilityHigh dielectric strengthExcellent chemical and abrasion resistanceThermoformableProduct available in widths up to 60"Product available with thicknesses from.. |
|||
CTE, linear | 119 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
CTE, linear | 119 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
CTE, linear | 119 µm/m-°C | 66.1 µin/in-°F | Above Tg |
Tra-Con Tra-Cast 3110 Low Density Epoxy Casting System TRA-CAST 3110 is a unicellular, low density, syntactic-foam epoxy resin casting system of medium viscosity that easily handles, mixes and cures at room temperature. Developed for industrial encapsul.. |
|||
CTE, linear | 119 µm/m-°C @Temperature -40.0 - 176 °C |
66.0 µin/in-°F @Temperature -40.0 - 349 °F |
ASTM D696 |
Entec Hylac® EX18 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
CTE, linear | 119 - 144 µm/m-°C | 66.0 - 80.0 µin/in-°F | ASTM D696 |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
CTE, linear | 119 - 144 µm/m-°C | 66.0 - 80.0 µin/in-°F | ASTM D696 |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
CTE, linear | 119 - 144 µm/m-°C | 66.0 - 80.0 µin/in-°F | ASTM D696 |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
CTE, linear | 119 - 144 µm/m-°C | 66.0 - 80.0 µin/in-°F | ASTM D696 |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
CTE, linear | 119 - 144 µm/m-°C | 66.0 - 80.0 µin/in-°F | ASTM D696 |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
CTE, linear | 119 µm/m-°C @Temperature 20.0 °C |
66.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-65D Polyester based. Excellent oil and chemical resistance. Applications include: Caster wheels, Seals, Gaskets, Animal tags, Hose jacketing, Ski boots, AutomotiveDat.. |