Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 106 µm/m-°C @Temperature 20.0 °C |
59.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
CTE, linear | 106 µm/m-°C @Temperature 20.0 °C |
59.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (DAM) Information provided by Ravago. |
|||
CTE, linear | 106 µm/m-°C @Temperature -30.0 - 80.0 °C |
58.9 µin/in-°F @Temperature -22.0 - 176 °F |
Borealis Method |
Borealis HK030U Polypropylene Compound HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit.. |
|||
CTE, linear | 106 µm/m-°C @Temperature 20.0 °C |
58.9 µin/in-°F @Temperature 68.0 °F |
|
Trelleborg Emerson & Cuming Stycast® E1410 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
CTE, linear | 106 µm/m-°C | 58.9 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® E3001-6 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E3001-HV is a snap cure, single component, silver-filled die attach adhesive for semiconductor plastic IC packaging. Also available in a frozen syringe. Advantages & .. |
|||
CTE, linear | 106 µm/m-°C @Temperature -30.0 - 30.0 °C |
58.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8350 HS BK-102 PA6 (Dry) Ultramid 8350 HS BK-102 is a type 6, black pigmented, impact modified graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness
combined with a.. |
|||
CTE, linear | 106 µm/m-°C @Temperature -30.0 - 30.0 °C |
58.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8350 HS PA6 (Dry) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
CTE, linear | 106 µm/m-°C | 58.9 µin/in-°F | ASTM E831 |
BASF Ultramid® 8351 HS BK 102 PA6 (Dry) Description: Ultramid 8351 HS BK-102 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughn.. |
|||
CTE, linear | 106 µm/m-°C | 58.9 µin/in-°F | ASTM E831 |
BASF Ultramid® 8351 HS BK 106 PA6 (Dry) Description: Ultramid 8351 HS BK-106 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughn.. |
|||
CTE, linear | 106 µm/m-°C @Temperature 20.0 °C |
58.9 µin/in-°F @Temperature 68.0 °F |
ASTM data |
BASF Capron® 8351 HS BK-102 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8351 HS BK-102 is a heat stabilized, pigmented black type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughness combined with a moderate fle.. |
|||
CTE, linear | 106 µm/m-°C @Temperature 20.0 °C |
58.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical HF-380 ABS, High Flow, High Impact Feature: Injection Molding, High FlowApplication: Electric & Electronic Products, Toys, Miscellaneous Goods)CAS No. 9003-56-9Information Provided by LG Chem |