Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 51 mm/min | 2.0 in/min | FM VSS-302 |
Multibase Multi-Flex® G 7705 TPE Styrene Ethylene Butylene Styrene Block Copolymer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Flame Spread | 51 mm/min | 2.0 in/min | FMVSS 302 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | FMVSS 302 |
A. Schulman PP 1930L-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930L-01 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided b.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | FMVSS 302 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | FMVSS 302 |
A. Schulman PP 1930L-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930L-01 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided b.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | FMVSS 302 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | FMVSS 302 |
A. Schulman PP 1930L-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930L-01 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided b.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | FMVSS 302 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | FMVSS 302 |
A. Schulman PP 1930L-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930L-01 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided b.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | FMVSS 302 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | FMVSS 302 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flame Spread | 50 mm/min @Thickness 1.00 mm |
2.0 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Crastin® SK642FR BK851 Polybutylene Terephthalate (PBT) 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR BK851 is a black 15% glass fiber reinforced flame retardant polybutylene terephthalate for injection molding. It has a.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | burn rate |
AlphaGary Evoprene™ LF 6160 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | burn rate |
AlphaGary Evoprene™ LF 6158 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | FMVSS 302 |
A. Schulman PP 1930L-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930L-01 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided b.. |
|||
Flame Spread | 51 mm/min | 2.0 in/min | FMVSS 302 |
A. Schulman PP 1930L-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930L-01 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided b.. |