Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Crastin® SK642FR BK851 Polybutylene Terephthalate (PBT)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® SK642FR BK851 Polybutylene Terephthalate (PBT).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR BK851 is a black 15% glass fiber reinforced flame retardant polybutylene terephthalate for injection molding. It has a UL94 V-0 rating @ 0.75mm.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ISO 527-1/-2
Elongation at Break 3.4 %
3.4 %
ISO 527-1/-2
Tensile Modulus 7.20 GPa
1040 ksi
ISO 527-1/-2
Flexural Strength 155 MPa
22500 psi
ISO 178
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 218 °C
424 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 203 °C
397 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
IEC 60695-11-10
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
Flame Spread 50 mm/min

@Thickness 1.00 mm
2.0 in/min

@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 32 %
32 %
ISO 4589-1/-2
Descriptive Properties Value Comments
Part Marking Code >PBT-GF15FR(17)<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PBT-GF15FR(17)
UL recognition UL
Users viewing this material also viewed the following: