Thermal Properties Metric English Comments
Flame Spread 30 mm/min
1.2 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 30 mm/min
1.2 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast MP 1.25 (UL 752 Level 1) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 30 mm/min
1.2 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast Poly 900 (DTD-5592-UK) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 30 mm/min
1.2 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast Poly II (Mil-P-5425) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 30 mm/min
1.2 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast SAR HP 1.25 (UL 752 Level 3) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 30 mm/min
1.2 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast Solarcryl (0.187") Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 30 mm/min
1.2 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast UF3 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 30 mm/min
1.2 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast UF4 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 30 mm/min
1.2 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast UF96 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 30 mm/min
1.2 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast UVT (Ultra-Violet Transmitting) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 30 mm/min
1.2 in/min
FMVSS302
Polyram Polytron P30N11 Polypropylene, 30% Long Fiber Glass
A chemically coupled 30% long fiber glass reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram.
Flame Spread 30 mm/min
1.2 in/min
FMVSS302
Polyram RamSter PF306G6 PBT, 30% Glass Fiber
30% Glass fiber reinforced, low viscosity PBT for injection molding applications.Information provided by Polyram.
Flame Spread 30 mm/min
1.2 in/min
FMVSS302
Polyram Polytron P30B07 Polypropylene, 30% Long Glass Fibers, UV Stabilized
A chemically coupled 30% long glass fibers reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.
Flame Spread 30 mm/min

@Thickness 1.00 mm
1.2 in/min

@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
DuPont Performance Polymers Crastin® HR5330HF BK503 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
Flame Spread 30 mm/min

@Thickness 1.00 mm
1.2 in/min

@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK261 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 for injection molding. It has excellent surface app..
Flame Spread 30 mm/min

@Thickness 1.00 mm
1.2 in/min

@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by..
Flame Spread 30 mm/min
1.2 in/min
Horizontal Burn Rate; FMVSS302
Asahi Kasei Thermylene® P6-30FM-0378 30% Glass/Mineral Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flame Spread 30 mm/min
1.2 in/min
Horizontal Burn Rate; FMVSS302
Asahi Kasei Thermylene® P6-25FG-0687 25% Glass Fiber Reinforced
Information provided by Asahi Thermofil
Flame Spread 30 mm/min
1.2 in/min
Horizontal Burn Rate; FMVSS302
Asahi Kasei Thermylene® P6-30FG-0632 30% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil