Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 93.0 °C | 199 °F | |
LG Chemical P.F.O Structure & Characteristics: Obtained as a by-product of naphtha pyrolysis process. Compared to other products, it is higher in density and significantly more viscous but lower in vapor pressureUses.. |
|||
Flash Point | 93.0 °C | 199 °F | |
Lord Adhesives 309 General Purpose, Non-Sag, Thixotropic Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 320 Resin; Closed Cup |
Lord Adhesives 320 / 322 Epoxy Adhesive LORD® 320/322 adhesive is a general purpose, two component epoxy adhesive system formulated for primerless adhesion to automotive sheet molded compounds (SMC). This adhesive system also provides .. |
|||
Flash Point | 93.0 °C | 199 °F | |
Lord Adhesives 360 Sag-Resistant, High-Performance, 5 min Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | A Resin; Closed Cup |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | B Curative; Closed Cup |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | C Curative; Closed Cup |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | D Curative; Closed Cup |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | E Curative; Closed Cup |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | K3425B; Setaflash, Closed Cup; ASTM D3278-82 |
Lord Adhesives Aeroglaze® K3425 Sandable Primer/Surfacer For application on epoxy graphite or other plastic substrates or over a suitable primer on metal.Limitations - Aeroglaze® K3425 primer/surfacer contains no inhibiting pigments and is not suitable.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | Seta |
Lord Adhesives Chemlok® 610 Adhesive Chemlok® 610 is an aqueous adhesive used to bond fluoroelastomers, polyacrylates, ethylene acrylic and peroxide vulcanizing EPDM elastomers. Chemlok 610 aqueous adhesive can also be used as a coa.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | |
Lord Adhesives CircuitSAFâ„¢ MA-420 Epoxy Surface Mount Adhesive CircuitSAFâ„¢ MA-420 is an epoxy surface mount adhesive that cures rapidly at elevated temperatures and has been designed for use in high speed printed circuit board assembly for the attachment o.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | Fusor 2201; Closed Cup |
Lord Adhesives Fusor® 2200 / 2201 Urethane Adhesive Fusor® 2200/2201 is a black equal-mix, twocomponent, paste urethane adhesive system. Fusor 2200/2201 adhesive bonds FRP, SMC, and other plastics with little surface preparation where bond strengt.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 309-2D Hardener; Closed Cup |
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | Mixed; Closed Cup |
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 310A Resin; Closed Cup |
Lord Adhesives Fusor® 310 A/B Epoxy Adhesive Lord® 310 adhesive is a modified, thixotropic, two-part epoxy adhesive which bonds well to many types of prepared metals, prepared rubber, urethane, and plastics. Originally formulated for primer.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 310B Hardener; Closed Cup |
Lord Adhesives Fusor® 310 A/B Epoxy Adhesive Lord® 310 adhesive is a modified, thixotropic, two-part epoxy adhesive which bonds well to many types of prepared metals, prepared rubber, urethane, and plastics. Originally formulated for primer.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 254 Hardener; Closed Cup |
Lord Adhesives Versilok® 265 / 254 Acrylic Adhesive LORD Versilok® 265/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | |
Solvay GEROPON® TC 42 LQ Surfactant Description: Liquid Sodium Methyl Cocoyl Taurate that demonstrates good lathering properties in skin cleanser and shampoo applications. Displaysexcellent dispersiblity properties in hard water and h.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | Closed cup |
Dow Corning AMS-C30 Cosmetic Wax A 70°C (158°F) melting point alkyl methyl siloxane wax. By modifying polydimethylsiloxane with a high molecular weight hydrocarbon, this wax exhibits characteristics typical of silicones and hydro.. |
|||
Flash Point | 93.0 °C | 199 °F | Closed Cup |
Dow Corning XIAMETER® PMCPPMX-0246 Cyclohexasiloxane Is chemically equivalent to DOW CORNING® 246 FLUID. This product is a volatile, low viscosity cyclohexasiloxane fluid for use in skincare, suncare, color cosmetics, hair care, and antiperspirant / .. |
|||
Flash Point | 93.0 °C | 199 °F | closed cup |
Dow Corning Z-1223 DIPHENYLDICHLOROSILANE Information provided by Dow Corning |
|||
Flash Point | >= 93.0 °C | >= 199 °F | Closed cup |
Dow Corning 203 Fluid 100% active alkylaryl polysiloxane fluid.Information provided by Dow Corning |
|||
Flash Point | 93.0 °C | 199 °F | Closed cup |
Dow Corning 230 Fluid 100% active alkylaryl polysiloxane fluid.Information provided by Dow Corning |
|||
Flash Point | >= 93.0 °C | >= 199 °F | Closed cup |
Dow Corning 2502 Cosmetic Fluid A linear polydimethylsiloxane with randomly distributed alkyl chains for use in skincare, woundcare, haircare, suncare, and color cosmetic applications.Information provided by Dow Corning |
|||
Flash Point | 93.0 °C | 199 °F | |
3M 32661 Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Flash Point | 93.0 °C | 199 °F | |
BASF Lupragen® DMI 1,2-Dimethyl Imidazole Formula: C5H8N2CAS: 1739-81-0Description: 1,2-Dimethylimidazole is a colorless to yellowish solid with an amine-like odor. Synonyms: DMI, 1,2-Dimethyl-1H-imidazolApplications: It is used as a Cataly.. |
|||
Flash Point | 93.0 °C | 199 °F | |
3M 32665 Green Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Flash Point | 93.0 °C | 199 °F | |
3M 32666 Tan Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Flash Point | 93.0 °C | 199 °F | |
3M 32663 Medium Grey Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |