Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 274 °C | 525 °F | |
Lubriplate L0750 Heat Transfer Oil Specialty Oil and Fluid These high flash and fire point oils are designed for exceptional heat transfer properties. For use on oil type heat exchangers in asphalt plants, roofer tar kettles, curing machines. Available in I.. |
|||
Flash Point | 274 °C | 525 °F | |
Lubriplate L0751 Heat Transfer Oil Specialty Oil and Fluid These high flash and fire point oils are designed for exceptional heat transfer properties. For use on oil type heat exchangers in asphalt plants, roofer tar kettles, curing machines. Available in I.. |
|||
Flash Point | 274 °C | 525 °F | |
Lubriplate L0757 Heat Transfer Oil Specialty Oil and Fluid These high flash and fire point oils are designed for exceptional heat transfer properties. For use on oil type heat exchangers in asphalt plants, roofer tar kettles, curing machines. Available in I.. |
|||
Flash Point | 274 °C | 525 °F | |
Lubriplate 220 SYN High Temp 100% Ester-Based Multi-Purpose Synthetic Fluid These 100% ester-based synthetic lubricants are recommended for applications that are exposed to high operating temperatures and must maintain a clean lubricated surface. Available in ISO viscosity .. |
|||
Flash Point | 274 °C | 525 °F | |
Teknor Apex TruVis Esters™ TNTM TriNonyl Trimellitate |
|||
Flash Point | 274 °C | 525 °F | ASTM D92 |
ExxonMobil Teresstic 150 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Flash Point | 274 °C | 525 °F | ASTM D92 |
ChevronTexaco Clarity® ISO 150 Saw Guide Oil FeaturesChevron Clarity Saw Guide Oils are designed to promote longer saw guide and saw blade life in thin kerf saw equipment, when operating in severe service and reduced cooling water modes.Chevro.. |
|||
Flash Point | 274 °C | 525 °F | ASTM D92 |
ChevronTexaco Delo® NLGI 0 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Flash Point | 274 °C | 525 °F | ASTM D92 |
ChevronTexaco Delo® NLGI 1 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Flash Point | 274 °C | 525 °F | ASTM D92 |
ChevronTexaco Delo® NLGI 2 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Flash Point | 274 °C | 525 °F | ASTM D92 |
ChevronTexaco NLGI 0 Ultra Duty Grease EP FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar.. |
|||
Flash Point | 274 °C | 525 °F | COC; ASTM D92 |
ExxonMobil Exterex™ TM111 Synthetic Fluid Product Description: Esterex™ Tirmellitate Esters are API category Group V fluids. These esters have excellent low-temperature properties, good lubricating properties and low volatilities. Esterex™.. |
|||
Flash Point | 274 °C | 525 °F | ASTM D92 |
ChevronTexaco NLGI 1 Ultra Duty Grease EP FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar.. |
|||
Flash Point | 274 °C | 525 °F | ASTM D92 |
ChevronTexaco NLGI 2 Ultra Duty Grease EP FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar.. |
|||
Flash Point | 274 °C | 525 °F | |
ChevronTexaco Starguide™ ISO 150 Texaco Starguide oils deliver value through:Cleaner cutting — Reduce excessive drag that slows cutting.Exceptional performance for low water and low oil consumption saw systems.Excellent low temper.. |
|||
Flash Point | 274 °C | 525 °F | ASTM D92 |
ExxonMobil Teresstic 150 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Flash Point | 274 °C | 525 °F | |
ConocoPhillips Synterra™ 3 Hydraulic Oil, AGMA No.3 Description: Conoco Synterra Environmental Fluids Hydraulic and Circulating Oils give outstanding protection to equipment and the environment. These oils are made from synthetic polyol ester fluids .. |
|||
Flash Point | 274 °C | 525 °F | |
BASF Palamoll® 656 Polymeric Plasticizer Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro.. |
|||
Flash Point | 274 °C | 525 °F | ASTM D92 |
ChevronTexaco Ulti-Plex® NLGI 0 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |
|||
Flash Point | 274 °C | 525 °F | ASTM D92 |
ChevronTexaco Ulti-Plex® NLGI 1 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |
|||
Flash Point | 274 °C | 525 °F | ASTM D92 |
ChevronTexaco Ulti-Plex® NLGI 2 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |