Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 71.0 - 175 °C | 160 - 347 °F | Average value: 100 °C Grade Count:67 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 - 175 °C | 311 - 347 °F | ISO 75 Af |
Vyncolit 4221 XB Novolac Phenolic Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 - 175 °C | 311 - 347 °F | ISO 75 A |
Vyncolit 4451 XB Novolac Phenolic Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 - 175 °C | 286 - 347 °F | Average value: 164 °C Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 - 175 °C | 149 - 347 °F | Average value: 149 °C Grade Count:125 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 85.0 - 175 °C | 185 - 347 °F | Average value: 154 °C Grade Count:17 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |