Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 37.3 °C | 99.1 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0735-U Hexene MDPE Rotational Molding Resin Good impact resistance, Excellent processabilityApplications: Toys, Complex custom parts, Home and garden items, MailboxesAdditives: Processing antioxidants, UV stabilizersInformation provided by NO.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.3 °C | 99.1 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin Features: Good impact properties Excellent processabilityNSF listed for Stds. 14, 24 and 61 Applications: ToysComplex custom partsHome and garden itemsMailboxesInformation provided by Nova Chemicals.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.3 °C | 99.1 °F | ASTM D648 |
NOVA Chemicals Novapol® PR-0636-UG Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.3 °C | 99.1 °F | ASTM D648 |
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.3 - 41.0 °C | 99.1 - 106 °F | Average value: 38.4 °C Grade Count:12 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.3 °C | 99.1 °F | ASTM D648 |
NOVA Chemicals Sclair® TD-7915-U Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.3 - 42.0 °C | 99.1 - 108 °F | Average value: 40.4 °C Grade Count:3 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.3 °C | 99.1 °F | ASTM D648 |
NOVA Chemicals Novapol® PR-0636-U Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |