Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | ASTM D648 |
RheTech Products G13P100-724UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, NH220L Clear Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 6.40 mm |
270 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 104R PC (Asia Pacific) LEXAN 104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 6.40 mm |
270 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® 133 PC (Asia Pacific) Nonhalogenated. 3.5 MFR. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 6.40 mm |
270 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 223S PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 6.40 mm |
270 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 943 PC Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 6.40 mm |
270 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 943ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Asia Pacific) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 3.20 mm |
270 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® FXD103R PC FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | ASTM D648 |
Ravago Manufacturing Americas Hylex® P1010L Polycarbonate, Unreinforced, Intermediate Flow Information provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 6.40 mm |
270 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® IR2840 PC 7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant, natural only.Effective January 15th, 2007 this grade will no longer be supported with biocompatibilit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 6.40 mm |
270 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® OQ4320R PC (Asia Pacific) Optical grade with UV cut-off up to 400 nm; greater optical purity than standard grades. For sunglass and sunvisor markets. Internal mold release. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 6.40 mm |
270 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® RL7517 PC FDA compliant (color limited). 2.5 MFR. Potable water/extrusion blowmolding applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | ASTM D648 |
RheTech Products G20P100-601 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUA5) Dark Graphite Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 6.40 mm |
270 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® 151 PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 6.40 mm |
270 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific) Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® XHT1141 PC (Europe-Africa-Middle East) XHT1141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | |
Lehmann & Voss LUVOCOM® 50/TF/15/BK Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 3.20 mm |
270 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON DX98477 PC LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | ASTM D648 |
Spartech Sungard Ultra Weatherable Polycarbonate Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | unannealed, .125in; ASTM D648 |
Star Plastics PC1510RUV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | unannealed, .125in; ASTM D648 |
Star Plastics PC1510UV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | ASTM D648 |
Samyang Trirex® 3017PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017PJ is a super high flow grade.Information provided by Samyang. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PC FR HS GY154 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and UV StabilizerFeatures: Flame Retardant and Heat StabilizedAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PC FR RD064 Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: RedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C @Thickness 3.20 mm |
270 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GFN1410V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1410V resin is a blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 10 % glass reinforcement. The resin is suitable for injection molding. Noryl GFN1410V resin has.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-10FG-Y950 10% Glass Fiber Reinforced, Lubricated Information provided by Asahi Thermofil |