Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 48.9 - 210 °C | 120 - 410 °F | Average value: 78.9 °C Grade Count:49 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 120 - 210 °C | 248 - 410 °F | Average value: 149 °C Grade Count:17 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 - 210 °C | 122 - 410 °F | Average value: 169 °C Grade Count:8 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.8 - 210 °C | 145 - 410 °F | Average value: 72.8 °C Grade Count:19 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.2 - 210 °C | 180 - 410 °F | Average value: 159 °C Grade Count:5 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 55.0 - 210 °C | 131 - 410 °F | Average value: 101 °C Grade Count:29 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |