Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.22 °C
180.0 °F
ASTM D648
Lucent Polymers ABS-45T Acrylonitrile Butadiene Styrene, High Impact
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.22 °C
180.0 °F
ASTM D648
Lucent Polymers PC/PBT-0820 Polycarbonate+PBT, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.22 °C
180.0 °F
ASTM D648
Lucent Polymers PC/PBT-1020 Polycarbonate+PBT, General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.22 °C
180.0 °F
ASTM D648
Lucent Polymers TPP-140 Polypropylene, Homopolymer, 40% Talc Filled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.