Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | Unannealed; ASTM D648 |
Multibase Nylex™ 2185 HF Polyamide + PP Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | ASTM D648 |
Nylene® 321 (HS) Impact Modified Nylon 6 Description: Nylene® 321 (HS) is an impact modified nylon 6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporatio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifaxâ„¢ HSBMG265 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ HSBMG265 medium high melt flow, 1,400 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of rigidity, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | ISO 75-2/A |
ExxonMobil AP3N Polypropylene Impact Copolymer Product Description: A medium impact copolymer resin designed for appliance applications requiring good stiffness and fast cycle time.Availability: Asia Pacific Features:Fast Molding CycleHigh Glos.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | ISO 75-2/A |
ExxonMobil Exxtral™ BMU 141 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive instrument panels in which good surface finish, high s.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | ISO 75-2/A |
ExxonMobil Exxtral™ BMU 234 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact and good dimensional stability.Availability: Africa & Middle Ea.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | ISO 75-2/A |
ExxonMobil Exxtral™ BMV 301 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, designed for automotive interior application in which good surface finish, high s.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CNU 017 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by high flow, high stiffness, low odor and emissions that is typically used automotive air conditioning units.Availabili.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | ISO 75-2/A |
ExxonMobil PPT0170F Polypropylene Homopolymer Product Description: PPT0170F is an unstabilized homo polymer granular resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation prov.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | ISO 75-2/A |
ExxonMobil PPU0180F Polypropylene Homopolymer Product Description: An unstabilized homopolymer granular resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation provided by Exxon.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | |
Aclo Accutech Polypropylene Copolymer CP0437M20L Mica Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | |
Aclo Accutech Polypropylene Copolymer CP0437T20L1 Talc Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | |
Aclo Accutech Polypropylene Copolymer CP0437T30L Talc Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.9 °C | 129 °F | ISO 75-2/A |
ExxonMobil PP7064L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with medium flow, high stiffness and antistatic properties. It is suitable for molding applications like consumer products, closures, contain.. |