Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA4/6 GF45 HS BK 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackTPCI# 9627150Informat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PEEK CF30 HF 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PEEK GF30 HF 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® TPX-HTN-01092 A 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® TPX-HTN-02028 A 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; Flatwise; ISO 75-2/A |
Solvay Specialty Polymers Amodel® A-6135 NL Polyphthalamide (PPA), 35% Glass Fiber Reinforcement
(discontin Amodel A-6135 NL polyphthalamide (PPA), a 35% glass reinforced, high-glow, non-lubricated, hot-water moldable resin specially designed for laser welding. The black version is a laser absorber, and t.. |