Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | >= 190 °C | >= 374 °F | ISO 75-C |
Raschig Group 2557 AMC Polyester Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low .. |
|||
Deflection Temperature at 8.0 MPa | 190 °C | 374 °F | ISO 75-2 |
Hexion Bakelite™ PF 6506 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures, UL Listed
&nbs Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant, UL listed molding compound 1.5 mm/V-.. |
|||
Deflection Temperature at 8.0 MPa | 190 °C | 374 °F | ISO 75-1/-2 |
Lanxess Durethan® DP BKV 60 H2.0 EF 900116 Nylon 6, 60% Glass Fiber PA 6, injection molding grade, 60% glass fibers, low viscosity, good flowability (Easy Flow), good heat-resistanceApplication Examples: gearbox housings, spring holders, automotive door handles |
|||
Deflection Temperature at 8.0 MPa | 190 °C | 374 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® AG-30 H PA66 Product description: Grilon AG-30 H black 9836 is a normal viscosity, specially heat stabilized PA 66 injection molding grade with 30% glass fibres. Grilon AG-30 H black 9836 has the following impor.. |
|||
Deflection Temperature at 8.0 MPa | 190 °C | 374 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BG-60 FC PA6-GF60 Product description: Grilon BG-60 FC is a heat stabilized PA6 injection molding grade with 60% glass fibers. Grilon BG-60 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
Deflection Temperature at 8.0 MPa | 190 °C | 374 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30 Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr.. |
|||
Deflection Temperature at 8.0 MPa | 190 °C | 374 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30 Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr.. |
|||
Deflection Temperature at 8.0 MPa | 190 °C | 374 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40 Product description: Grivory XE 4101 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Deflection Temperature at 8.0 MPa | 190 °C | 374 °F | HDT/C; ISO 75-2 |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |