Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 725 °C @Thickness 2.00 mm |
1340 °F @Thickness 0.0787 in |
Ignition Temperature; IEC 60695-2-13 |
PolyOne OnFlex™ S HF 50A-3S1981 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Glow Wire Test | 725 °C @Thickness 2.00 mm |
1340 °F @Thickness 0.0787 in |
Ignition Temperature; IEC 60695-2-13 |
PolyOne OnFlex™ S HF 70A-3S1984 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Glow Wire Test | 725 °C @Thickness 2.00 mm |
1340 °F @Thickness 0.0787 in |
Ignition Temperature; IEC 60695-2-13 |
PolyOne OnFlex™ S HF 90A-3S1988 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Glow Wire Test | 725 °C @Thickness 1.60 mm |
1340 °F @Thickness 0.0630 in |
Ignition Temperature; IEC 60695-2-13 |
PolyOne Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Glow Wire Test | 725 °C @Thickness 0.710 mm |
1340 °F @Thickness 0.0280 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66
(Unverified Data**) Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 725 °C @Thickness 0.710 mm |
1340 °F @Thickness 0.0280 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66
(Unverified Data**) Zytel® 103FHS BKB009 is a heat stabilized, internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Perf.. |
|||
Glow Wire Test | 725 °C @Thickness 1.50 mm |
1340 °F @Thickness 0.0591 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 725 °C @Thickness 0.710 mm |
1340 °F @Thickness 0.0280 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 725 °C @Thickness 1.00 mm |
1340 °F @Thickness 0.0394 in |
GWIT |
LATI Latamid 66 H2 G/35-V0KB3 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Glow Wire Test | 725 °C @Thickness 1.00 mm |
1340 °F @Thickness 0.0394 in |
GWIT; IEC 60695-2-13 |
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme.. |
|||
Glow Wire Test | 725 °C @Thickness 2.00 mm |
1340 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Glow Wire Test | 725 °C @Thickness 1.00 mm |
1340 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature, dry; IEC 60695-2-13 |
DSM Akulon® K222-KMV5 /A PA6-MD25 FR(30) 25% Mineral Reinforced, Flame Retardant (Halogen free), Color Stabilized |
|||
Glow Wire Test | 725 °C @Thickness 0.750 mm |
1340 °F @Thickness 0.0295 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Glow Wire Test | 725 °C @Thickness 1.50 mm |
1340 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
DSM Arnite® TV4 230 SF PBT-15% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glow Wire Test | 725 °C @Thickness 2.00 mm |
1340 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecodur® PB70 GR20 BK002 TD21 PBT/PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), impact modified, natural Information provided by Eurotec® |
|||
Glow Wire Test | 725 °C @Thickness 2.00 mm |
1340 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecodur® PB70 GR30 NL SV20 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr.. |
|||
Glow Wire Test | 725 °C @Thickness 1.50 mm |
1340 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Glow Wire Test | 725 °C @Thickness 0.750 mm |
1340 °F @Thickness 0.0295 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Glow Wire Test | 725 °C @Thickness 0.750 mm |
1340 °F @Thickness 0.0295 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Glow Wire Test | 725 °C @Thickness 1.50 mm |
1340 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Glow Wire Test | 725 °C @Thickness 2.00 mm |
1340 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Glow Wire Test | 725 °C @Thickness 1.00 mm |
1340 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |