Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJCK504L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Polimeri Europa Eraclene® BB 76 High Density Polyethylene - Blow Molding Eraclene BB 76 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 30 liters.Er.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | TPE-0089 (ASTM D 746) |
ExxonMobil Vyram™ 9271-65 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D696 |
NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D696 |
NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Eastman E6838-850P Polyethylene
(discontinued **) E6838-850P is a low density resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seal.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Chevron Phillips HiD® 9720 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: good flow, moderate impact strength, excellent stiffness, moderate ESCR, moderate shrinkage resistanceApplications: pails, structural foamInformation p.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | |
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray RTV 157 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | |
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | |
Momentive Performance Materials RTV162 Electronic Grade Silicone Adhesive Sealant, White RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | |
Momentive Performance Materials RTV5818 One-Component, Modified Alkoxy Adhesive Sealant, Translucent RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Teknor Apex ELEXAR® EL 8451 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex Telcar® TELC 302 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex UNIPRENE® 7100-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | JIS K6301 |
Toyobo Pelprene™ P-280B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
ExxonMobil Paxon™ FD60-018 Compression Molding Resin FD60-018 is a very high molecular weight high density polyethylene powder. It exhibits very high impact strength.Information provided by ExxonMobil Chemical |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
ExxonMobil Santoprene® 271-55 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Alliance Polymers Viprene™ G55A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G55A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D 746 |
AlphaGary Evoprene™ LF 6156 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | |
Teknor Apex Elexar® EL 3954-80 Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical properti.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Teknor Apex ELEXAR® EL 8732 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | TPE-0089 (ASTM D 746) |
Advanced Elastomer Systems Santoprene® 281-64 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
PolyOne Synprene® RT-3890M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
LG Chemical LC175 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |