Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W3200 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W3204 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJJC34L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | <= -20.0 °C | <= -4.00 °F | ASTM D746 |
Polimeri Europa Riblene® MR 10 Low Density Polyethylene - Injection Molding Riblene MR 10 is a high fluidity low density polyethylene resin (LDPE).Parts made with Riblene MR 10 are characterized by a high flexibility.Main Applications: Riblene MR 10 is suitable for injecti.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible A4D02 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible transparent PVC Compound designed primarily for indoor mats.Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3437 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
LyondellBasell Montell 8640 Polybutene-1 Key Features: semi-crystalline low ethylene content random copolymer, miscible with polypropylenes, FDA acceptableApplications: minor additive in a polyethylene peel seal layerMeets FDA requirements.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 3200-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 3301-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 4112 Polyvinyl Chloride, Flexible Notes: 75°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Mold.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 94-A0098A-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex Fireguard® 910L16-C6-NL1 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant; Low Smoke Emission Uses: Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC Article 760; NEC Ar.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 01-A0303E-95 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Uses: Automotive Electronics; Insulation; Wire and Cable Applications Wire Types: GPT Agency Ratings: SAE J1128 Forms: PelletsInformation Provided by Tekno.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P403J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfant articles, toys.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P702J Polypropylene Injection Molding Key Characteristics:High clarityHigh stiffnessGood processabilityMicrowavable for cooking applicationsOdorlessSafe for food contactRecommended Applications:General purpose injection parts that requi.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P740J Polypropylene Injection Molding Key Characteristics:Good flowabilityGood processabilityHigh stiffnessRecommended Applications:Automotive, motorcycle and electrical appliance parts that require good flowability such as automotive t.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P841J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsContains UV stabilizer and anti-static agentRecommended Applications:Electric.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P842J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityExcellent stiffnessSuitable for complex parts and large partsRecommended Applications:Electrical appliance parts, mainly for refriger.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 6820 Flexible PVC, Injection Molding for Footwear Soles |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 7516 Flexible PVC, Injection Molding for Footwear Soles |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PMS 75 Flexible PVC, Lead Free Gas pipes stabilized Ca-Zn |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Colorite Polymers CS1539GP Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Colorite Polymers CS8042SC Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Colorite Polymers CS9039UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | |
Colorite Polymers Self Frosting™ 9011SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 8202 Flexible PVC, Injection Molding for Footwear Soles |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | |
Colorite Polymers 9011 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D-746 |
Axiall 1131-57D Wire & Cable Flexible PVC Non-lead stabilized 105°C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | |
Aearo E-A-R Specialty Composites Isodamp® C-1000 Series TPE Isodamp® C-1000 Series TPEs feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protection f.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | |
AlphaGary PVC GM 8001-E Natural LCF Polyvinyl Chloride Thermoplastic A lead free, flame retarded, V-O rated compound designed for plug molding |