Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -59.0 °C | -74.2 °F | ASTM D746 |
PolyOne Elastamax™ HTE 3060 Polyvinyl Chloride + NBR (PVC+NBR) Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a.. |
|||
Brittleness Temperature | -59.0 °C | -74.2 °F | ASTM D746 |
Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips 7105T LLDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 214, A 35307Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips 7108T LLDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 214, A 35307Applications:Cast Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Containm.. |
|||
Brittleness Temperature | -59.0 °C | -74.2 °F | Bell |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips HiD® 9300 HDPE Orange Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234363E; ASTM D 4976 Classification: PE 225, A 56607Characteristics: PPI Recommended Hydrostatic Design Bases (HDB): 1250.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips HiD® 9301 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234360A; ASTM D 4976 Classification: PE 225, A 56607Applications:Base Resin for use in Gas, Oil Patch and Industrial Pipe.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips HiD® 9302 HDPE Yellow Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234363E; ASTM D 4976 Classification: PE 225, A 56607Applications:Natural Gas Distribution Piping and FittingsData provide.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips HiD® 9308 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 345460A; ASTM D 4976 Classification: PE 235, A 56607Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips HiD® 9326 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 335440A; ASTM D 4976 Classification: PE 235, A 56606Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips HiD® 9348 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 335440A; ASTM D 4976 Classification: PE 235, A 56606Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips HiD® 9396T HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips HiD® 9398T HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips HiD® 9642 HDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips HiD® 9646T HDPE High Molecular Weight Sheeting Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 4976 Classification: PE 235, A 56606Applications:Sheeting, Thermoforming, Profile ExtrusionData provided by Chevron Chemical. |
|||
Brittleness Temperature | -59.0 °C | -74.2 °F | ASTM D746 |
Teknor Apex Flexalloy® 3500-35 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Brittleness Temperature | -59.0 °C | -74.2 °F | ASTM D746 |
Teknor Apex Flexalloy® 3501-35-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Brittleness Temperature | -59.0 °C | -74.2 °F | ASTM D746 |
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581 Forms: Pellets Processing Method: Extrusion; Injection.. |
|||
Brittleness Temperature | -59.0 °C | -74.2 °F | Bell |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Brittleness Temperature | -59.0 °C | -74.2 °F | |
TSE Industries Millathane® CM High Temperature-Resistant Millable Polyester Polyurethane MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Brittleness Temperature | <= -59.0 °C | <= -74.2 °F | ASTM D746 |
Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification:345464C when used with an approved color concentrate; ASTM D 4976 Classification: PE 235, A 56607Applications:Pressure Pip.. |
|||
Brittleness Temperature | -59.0 °C | -74.2 °F | |
TSE Industries Millathane® CM High Temperature-Resistant Millable Polyester Polyurethane MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |