Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable JLK51L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3821 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Teknor Apex APEX® 155 Polyvinyl Chloride, Flexible Notes: 80°C Jacket; RoHS CompliantFeatures: Sunlight Resistant (720 hours); Good UV Resistance Uses: Building Wire Jacketing; Wire and Cable Applications Agency Ratings: UL QMTT2 .E73402Forms: Pe.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Teknor Apex APEX® 1700-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMForms-PelletsAppearance- Natural Color, OpaqueInformation provided by Teknor Apex Company |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Teknor Apex APEX® 2585-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Teknor Apex APEX® 3202-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Caps, Closure, Connectors, Food Service Applications, Safety Equipment, Valves/Valve Parts Appearance-Cl.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Teknor Apex APEX® 3302-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Teknor Apex APEX® 3610-80 Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: First Generation SeriesInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Teknor Apex APEX® 536 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Teknor Apex APEX® 88-N398-J Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Features: Low Gloss Uses: Communication Wire Jacketing Forms: Pellets Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 800; NEC Article 820; UL 13;.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Teknor Apex APEX® 2080-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-ClearForms-PelletsProcessing Method-Extrusi.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | |
Daikin DAI-EL G-501NK Fluoroelastomer Terpolymer, Diamine Curable Grade, 68% Fluorine Content Features: Good mechanical characteristics.Information provided by Daikin Industries. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GA 75/1 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Colorite Polymers CS6023GP Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Colorite Polymers CS8039UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | |
Colorite Polymers 7812 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | |
Colorite Polymers Self Frosting™ 7811SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | Impact Brittleness; ASTM D746 |
Bayshore Vinyl Compounds BVC 7200-75 Vinyl Compound BVC 7200-75 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a s.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D-746 |
Axiall 10840 Wire & Cable Flexible PVC High gloss jacket and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D-746 |
Axiall 2110 Wire & Cable Flexible PVC Tray cable jacket for 105°C applications. Also suitable for direct burial applications. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gu.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D-746 |
Axiall 830B Wire & Cable Flexible PVC 80°C rated compound recommended for UL 360, liquid tight flexible conduit jacket applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D-746 |
Axiall 8747 Moldings & Extrusions Flexible PVC Economical general purpose molding and extrusion compound with good flex whitening resistance especially in darker colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation i.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Colorite Polymers 6718 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | ASTM D746 |
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer Zythane™ 5085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | |
AlphaGary GW 2403-1 VW1 LCF Flame Retardant Polyvinyl Chloride 90°C rated jacket compound for tray cable, oil resistant |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | Plasticizer conc. in vinyl film 50 phr; ASTM D746 |
BASF Palatinol® N Diisononyl Phthalate Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | |
Colorite Polymers 7811 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Brittleness Temperature | -31.0 °C | -23.8 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 65/7 Flexible PVC, Lead Free Fuses |