Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 311DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Informatio.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SG910 HIPS High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SG960 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical HIPS 405AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=2.50 mm |
122 °F @Thickness >=0.0984 in |
|
LG Chemical HIPS 406AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical LI942 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical LI942 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical LUMAX HR5157 PBT+ABS+GF15%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF15%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 3.00 mm |
122 °F @Thickness 0.118 in |
|
Aardvark Polymers AARTEL® 2100UV Acetal Homopolymer Rotational Molding Resin Aartel 2100UV is a natural acetal homopolymer with UV stabilizers.Aartel 2100UV is a medium viscosity resin with excellent flow characteristics.Aartel 2100UV is available in natural white and may be.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical TR557 MABS, High Transparency, High Impact Feature: Injection Molding, High Transparency, High ImpactApplication: Electric/Electronic Applications, Copier, Printer etc.CAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical TR557 MABS, High Transparency, High Impact Feature: Injection Molding, High Transparency, High ImpactApplication: Electric/Electronic Applications, Copier, Printer etc.CAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness <=3.00 mm |
122 °F @Thickness <=0.118 in |
|
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness <=1.50 mm |
122 °F @Thickness <=0.0591 in |
|
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness <=3.00 mm |
122 °F @Thickness <=0.118 in |
|
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness Feature: Injection Molding, High Transparency, High Rigidity, High HardnessApplication: Electric/Electronic Parts Copier, Compact Cases etc.CAS No. 9011-14–7 and 9003-56-9Information provided b.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 3.00 mm |
122 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Hytrel® G3548L TPC-ET
(Unverified Data**) Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=6.00 mm |
122 °F @Thickness >=0.236 in |
|
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=6.00 mm |
122 °F @Thickness >=0.236 in |
|
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |