Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 311DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Informatio.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=1.50 mm |
194 °F @Thickness >=0.0591 in |
|
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=3.00 mm |
194 °F @Thickness >=0.118 in |
|
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=3.00 mm |
194 °F @Thickness >=0.118 in |
|
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=1.50 mm |
194 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN2101FC PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame RetardanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemi.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=1.50 mm |
194 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN2201FM PC+GF20%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF20%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=3.00 mm |
194 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN2201FM PC+GF20%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF20%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=1.50 mm |
194 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GP1006FM PC, Flame Retardant Description: Injection Molding, PC, Flame RetardantApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=3.00 mm |
194 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GP1006FM PC, Flame Retardant Description: Injection Molding, PC, Flame RetardantApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.00 mm |
194 °F @Thickness 0.0394 in |
UL 746 |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.50 mm |
194 °F @Thickness 0.0591 in |
UL 746 |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.50 mm |
194 °F @Thickness 0.0591 in |
UL 746 |
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.60 mm |
194 °F @Thickness 0.0630 in |
UL 746 |
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 40.6 mm |
194 °F @Thickness 1.60 in |
UL 746 |
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.10 mm |
194 °F @Thickness 0.0433 in |
UL 746 |
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.10 mm |
194 °F @Thickness 0.0433 in |
UL 746 |
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.10 mm |
194 °F @Thickness 0.0433 in |
UL 746 |
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.00 mm |
194 °F @Thickness 0.0394 in |
UL 746 |
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.50 mm |
194 °F @Thickness 0.0591 in |
UL 746 |
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.50 mm |
194 °F @Thickness 0.0591 in |
UL 746 |
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.00 mm |
194 °F @Thickness 0.0394 in |
UL 746 |
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 0.750 mm |
194 °F @Thickness 0.0295 in |
UL 746B |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.50 mm |
194 °F @Thickness 0.0591 in |
UL 746B |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746B |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 25.4 mm |
194 °F @Thickness 1.00 in |
UL 746 |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.00 mm |
194 °F @Thickness 0.0394 in |
UL 746 |
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.50 mm |
194 °F @Thickness 0.0591 in |
UL 746 |
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |