Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9320 BK851 PBT
(Unverified Data**) Crastin® LW9320 BK851 is a 20% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) Zytel® 70G30HSL BK039B is a 30% glass reinforced, heat stabilized, black nylon 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 0.710 mm |
257 °F @Thickness 0.0280 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 70G35HSL BK039B Nylon 66
(Unverified Data**) Zytel® 70G35HSL BK039B is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 70G35HSL BK039B Nylon 66
(Unverified Data**) Zytel® 70G35HSL BK039B is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL746B |
Mitsubishi Xantar® 18 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® 19 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL746B |
Mitsubishi Xantar® 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® F 23 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® F 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® FC 19 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® FC 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G4F 25 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® F 23 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® MX 2015 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-HG3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-HG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
|
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
|
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |