Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 6.00 mm |
239 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Crastin® S600F20 BK851 PBT
(Unverified Data**) Crastin® S600F20 BK851 is an unreinforced, lubricated, medium viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Crastin® S600F20 BK851 PBT
(Unverified Data**) Crastin® S600F20 BK851 is an unreinforced, lubricated, medium viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Crastin® S600F40 BK851 PBT
(Unverified Data**) Crastin® S600F40 BK851 is an unreinforced, lubricated, low viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 6.00 mm |
239 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 6.00 mm |
239 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Crastin® S620F20 BK851 PBT
(Unverified Data**) Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly.. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 6.00 mm |
239 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Crastin® SK601 BK851 PBT
(Unverified Data**) Crastin® SK601 BK851 is a 10% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Minlon® 10B140 BK061 Nylon 66
(Unverified Data**) Minlon® 10B140 BK061 is a 40% mineral reinforced, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness >=3.00 mm |
239 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness >=3.00 mm |
239 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1301EP30 Polycarbonate Resin Description: LUPOY PC 1301EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness >=1.50 mm |
239 °F @Thickness >=0.0591 in |
|
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 1.60 - 1.70 mm |
239 °F @Thickness 0.0630 - 0.0669 in |
|
LG Chemical Lupoy 1201HP-08 Polycarbonate Resin Description: LUPOY PC 1201HP-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 1.60 - 1.70 mm |
239 °F @Thickness 0.0630 - 0.0669 in |
|
LG Chemical Lupoy 1201HP-21 Polycarbonate Resin Description: LUPOY PC 1201HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness >=3.00 mm |
239 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1201HP-21 Polycarbonate Resin Description: LUPOY PC 1201HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 3.17 mm |
239 °F @Thickness 0.125 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 0.780 mm |
239 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 1.57 mm |
239 °F @Thickness 0.0618 in |
UL 746 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 3.17 mm |
239 °F @Thickness 0.125 in |
UL 746 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 1.57 mm |
239 °F @Thickness 0.0618 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 3.17 mm |
239 °F @Thickness 0.125 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 3.17 mm |
239 °F @Thickness 0.125 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 0.780 mm |
239 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 1.57 mm |
239 °F @Thickness 0.0618 in |
UL 746 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 3.17 mm |
239 °F @Thickness 0.125 in |
UL 746 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 3.17 mm |
239 °F @Thickness 0.125 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 1.57 mm |
239 °F @Thickness 0.0618 in |
UL 746 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 3.17 mm |
239 °F @Thickness 0.125 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 3.17 mm |
239 °F @Thickness 0.125 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 3.17 mm |
239 °F @Thickness 0.125 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 115 °C @Thickness 0.780 mm |
239 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |