Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 900 °C | 1650 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® FXD173R PC (Europe-Africa-Middle East) LEXAN FXD173R is a UV stabilized translucent high flow grade for light diffusion special effects. The color package may affect performance. |
|||
Glow Wire Test | 900 °C | 1650 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Glow Wire Test | 900 °C | 1650 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Glow Wire Test | 900 °C | 1650 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Glow Wire Test | 900 °C | 1650 °F | GWIT at 1.0 mm; IEC 60695-2-13 |
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant Vypet VNT 615 FR is a 15% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216.. |