Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics EXTEM UH1026 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 955A PC (Asia Pacific) Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 955AU PC (Europe-Africa-Middle East) Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Asia Pacific) LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER (Asia Pacific) Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm .. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Asia Pacific) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Asia Pacific) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL8134 PC COPOLYMER (Asia Pacific) Lexan* EXL8134 is a PC/siloxane copolymer resin with high flow, excellent low temperature impact and 30% post consumer recycle content. Limited availability and restricted color only. Higher color v.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL8454 PC COPOLYMER (Asia Pacific) Lexan* EXL8454 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 50% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL8483 PC COPOLYMER (Asia Pacific) Lexan* EXL8483 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 80% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific) 7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX2619 PC (Europe-Africa-Middle East) Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance. |
|||
Glow Wire Test | >= 875 °C | >= 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX2910T_ PC (Europe-Africa-Middle East) Global grade. LEXAN LUX2910T is an injection moulding grade especially designed for manufacturing optical parts requiring superior flow properties combined with very high transmission and color stab.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 925U PC (Europe-Africa-Middle East) Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 955A PC Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER (Asia Pacific) Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER (Asia Pacific) Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm.. |