Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 750 °C | 1380 °F | |
Plastcom SLOVASTER® B GF 40 PBT reinforced with 40% glass fibre Features: PBT for injection moulding, chemically reinforced with 40% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Glow Wire Test | 750 °C | 1380 °F | |
Plastcom SLOVASTER® B1 GF 6 HML PBT, 6% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Glow Wire Test | 750 °C @Thickness 1.00 mm |
1380 °F @Thickness 0.0394 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Cycoloy® C3100 PC+ABS (Europe-Africa-Middle East) C3100 is blow moulding/extrusion grade offering low temperature ductility, high heat resistance and high meltstrength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Glow Wire Test | 750 °C @Thickness 1.60 mm |
1380 °F @Thickness 0.0630 in |
IEC 695-2-1 |
Polykemi AB POLYblend 85E PC/ABS-Blend Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYblend 85FS GF10 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PP CQX30030 RTX Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPC T25020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH GF5030 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH TS15020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPHC GF3030 PD2 Polypropylene, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYshine PBT D221 PBT, Impact Modified Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYshine PBT D221 QF30 PBT, Glass and Mineral Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYshine PBT D231 GF15 PBT, Glass-Fiber Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB SCANMID 6 B12^ F Nylon 6 Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 0.750 mm |
1380 °F @Thickness 0.0295 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific) 7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Glow Wire Test | 750 °C @Thickness 3.00 mm |
1380 °F @Thickness 0.118 in |
IEC 60695-2-12 |
DuPont Performance Polymers Crastin® S620F20 BK851 PBT
(Unverified Data**) Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly.. |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PP EIP16020 F PP Mineral Reinforced, Extrusion Grade, Low CLTE Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH GF35040 D PP, Glass Fiber-Reinforced, Chemically Coupled, Detergent Resistant Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYlux 3809SLB PC/PBT-Blend, Paintable Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 3.20 mm |
1380 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Geloy CR7520 ASA (Europe-Africa-Middle East) Geloy CR7520 is a general purpose injection moulding grade, blend of ASA/SAN. It can be positioned for outside parts in various markets, such as telecommunication, transportation, B&C, lighting and .. |
|||
Glow Wire Test | 750 °C @Thickness 3.20 mm |
1380 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Glow Wire Test | 750 °C @Thickness 3.00 mm |
1380 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL WCP821U PPE-TPE (Asia Pacific) UV stabilized, halogen free Flexible Noryl injection molding grade for overmolding applications such as plugs, strain relief's, and connectors. Good color stability after UV weathering per ASTM D445.. |
|||
Glow Wire Test | 750 °C @Thickness 3.00 mm |
1380 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Europe-Africa-Middle East) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN.. |
|||
Glow Wire Test | 750 °C | 1380 °F | G.W.I.T.; IEC 60695 |
Polyram Polytron P30N11 Polypropylene, 30% Long Fiber Glass A chemically coupled 30% long fiber glass reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram. |
|||
Glow Wire Test | 750 °C | 1380 °F | 60695-2-10 |
Tisan TISARBON® UNR Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Glow Wire Test | 750 °C | 1380 °F | |
BLUESTAR 403HF-G20 PBT, 20% Glass Filled Typical Applications: Halogen Free; E/E connectors, socketsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH GF5035 PD2 VT Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled/Heat Resistant Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH TS15030 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | <= 750 °C @Thickness 3.00 mm |
<= 1380 °F @Thickness 0.118 in |
IEC 695 |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Glow Wire Test | 750 °C | 1380 °F | |
Polyram RamSter PF392G6 PBT, 30% Glass Fiber 30% glass-fiber reinforced, surface modified PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |