Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants 5301 (SVLG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants 572H-10 Dispersion Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants 716A (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants 716C (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants 716HT (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants 716L (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants 717E(RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8750 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8751 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8751R (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8980 (499) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8981 (899-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8981R (899RP-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8981S (899S-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8981SR (899S-1-RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8981X (899XP-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -67.0 °C | -88.6 °F | |
Teknor Apex TruVis Esters™ DIOA Di-IsoOctyl Adipate |
|||
Pour Point | -67.0 °C | -88.6 °F | |
Teknor Apex TruVis Esters™ DOA Di-Octyl Adipate |
|||
Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
Nye Lubricants 5300 (SVLG) Synthetic Oil Information provided by Nye Lubricants. |